Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 50 g/10 min @Load 2.16 kg, Temperature 230 °C |
50 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
Phillips 66 COPYLENE® CM500LN Polypropylene, Impact Copolymer, High Flow, Medium Impact, Nucleated, Lube, Injection Molding COPYLENE™ CM500LN is a very high melt flow, medium impact polypropylene copolymer resin, designed for injection molding applications requiring a good balance of properties with faster cycling capab.. |
|||
Melt Flow | 50 g/10 min @Load 2.16 kg, Temperature 190 °C |
50 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D 1238 |
Chevron Phillips Marlex® 1409 Injection Molding Resin
(discontinued **) Resin Type: Homopolymer; ASTM D 4976 Classification: PE 111, A 22200Characteristics: Good Flexibility, Excellent Flow, Excellent Warping Resistance, Excellent Mold Release, Moderate ESCRApplications.. |
|||
Melt Flow | 50 g/10 min @Load 2.16 kg, Temperature 275 °C |
50 g/10 min @Load 4.76 lb, Temperature 527 °F |
ASTM D1238 |
Solvay Specialty Polymers Halar® 1450LC Polyethylene, Chlorotrifluoroethylene (ECTFE)
(Unverified Data**) Information provided by Solvay Specialty Polymers. |
|||
Melt Flow | 50 g/10 min @Load 2.16 kg, Temperature 230 °C |
50 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
M. Holland Company CP850 Polypropylene Impact Copolymer Impact copolymerFast production cycleHigh flowHigh stiffnessApplications: ContainersHousehold goodsThin-walled parts |
|||
Melt Flow | 50 g/10 min @Load 2.16 kg, Temperature 230 °C |
50 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
LG Chemical KEYFLEX BT 3028D Ester Type TPE Description: Injection Molding, TPC-ET, Functional, Fast Molding, Low ModulusApplication: Automotive Interior, Soft Touch GripsCAS: 37282-12-5Information provided by LG Chemical |
|||
Melt Flow | 50 - 80 g/10 min | 50 - 80 g/10 min | Melt Volume Rate (cm³/10 min) |
Huntsman IROGRAN® A 85 P 4441 TPU-Polyether Introduction: IROGRAN A 85 P 4441 is a polyether based thermoplastic polyurethane intended for injection molding and extrusion applications. IROGRAN A 85 P 4441 is part of the HUNTSMAN technical ext.. |
|||
Melt Flow | 50 - 60 g/10 min @Load 2.16 kg, Temperature 235 °C |
50 - 60 g/10 min @Load 4.76 lb, Temperature 455 °F |
ASTM D1238 |
Gromax PBT 1200-211L Product Description: PBT unreinforced middle viscosity injection molding grade. Characteristics:Excellent electrical property Excellent temperature resistance, high heat distortion temperature. Exce.. |
|||
Melt Flow | 50 g/10 min @Load 5.00 kg, Temperature 266 °C |
50 g/10 min @Load 11.0 lb, Temperature 511 °F |
ASTM D1238 |
SABIC Innovative Plastics Valox® 4031 PBT (Europe-Africa-Middle East) VALOX 4031 is a 30% high strength glass fibre reinforced PBT injection moulding resin with excellent strength, stiffness and heat resistance. Applications: appliance handles, spotlights, electric mo.. |
|||
Melt Flow | 50 g/10 min @Load 2.16 kg, Temperature 330 °C |
50 g/10 min @Load 4.76 lb, Temperature 626 °F |
ASTM D1238 |
Samsung Cheil Industries Infino® TK-6036H PPA, Glass Filled Information provided by Samsung Cheil Industries. |
|||
Melt Flow | 50 g/10 min @Load 5.00 kg, Temperature 250 °C |
50 g/10 min @Load 11.0 lb, Temperature 482 °F |
ASTM D1238 |
Samyang Tribit® 1500G15 Polybutylene Terephthalate, 15% Glass Reinforced Characteristics:G/F reinforcedHeat and Impact resistantApplications:AutomotiveConnectorGearOutdoor handleIgnition systemElectronicConnectorGas valveCoil bobbinSwitch caseRelay caseO/A partsAll infor.. |
|||
Melt Flow | 50 g/10 min @Load 10.00 kg |
50 g/10 min @Load 22.05 lb |
ASTM D1238 |
Sumitomo Chemical ESPOLEX® 3785 Thermoplastic Elastomer ESPOLEX® TPE Series is a group of thermoplastic elastomers produced by Sumitomo Chemical Company. Among its material advantages, ESPOLEX® TPE Series is distinguished by offering many low-densi.. |
|||
Melt Flow | 50 g/10 min @Load 2.16 kg, Temperature 230 °C |
50 g/10 min @Load 4.76 lb, Temperature 446 °F |
ISO 1133 |
Borealis Bormed™ BH348MO Polypropylene Heteroplastic Copolymer for Injection Molding Bormed™ BH348MO is a polypropylene copolymer characterized by high impact strength, fast flow and crystallization speed. The material is nucleated with Borstar® Nucleation Technology (BNT). This .. |
|||
Melt Flow | 50 g/10 min @Temperature 230 °C |
50 g/10 min @Temperature 446 °F |
ASTM D1238 |
A. Schulman PP 3471-01 Polypropylene High Flow Homopolymer Polypropylene DescriptionPolypropylene PP 3471-01 is an ultra high flow homopolymer polypropylene designed for high speed, thin wall injection molding.Information provided by A. Schulman. |
|||
Melt Flow | 50 g/10 min @Load 2.16 kg, Temperature 190 °C |
50 g/10 min @Load 4.76 lb, Temperature 374 °F |
|
Wico Plast Wicotal 500 Acetal ApplicationsInjection moldingAll information provided by Wico Plast, Warenhandelsges. mbH |
|||
Melt Flow | 50 g/10 min @Temperature 230 °C |
50 g/10 min @Temperature 446 °F |
I<sub>2</sub>; ASTM D1238 |
Formosa Plastics Formolene® 6550A Thin Walled Injection Molding Polypropylene Impact CopolymerApplications: Housewares, containers and other rigid packaging.Formolene 6550A (DEVELOPMENTAL) is a medium impact, high flow, controlled rheology copolymer of polypropylene designed .. |
|||
Melt Flow | 50 g/10 min @Load 2.16 kg, Temperature 230 °C |
50 g/10 min @Load 4.76 lb, Temperature 446 °F |
ISO 1133 |
Total PPC 11750 Polypropylene, Heterophasic Copolymer, Injection Molding Polypropylene PPC 11750 is a nucleated and controlled-rheology heterophasic copolymer with very high Melt Flow index of 50 g/10 min.Polypropylene PPC 11750 is characterized by good impact resistance.. |
|||
Melt Flow | 50 g/10 min | 50 g/10 min | ASTM D1238 |
Total PPC 4944WZ Polypropylene, Impact Copolymer ATOFINA 4944 polypropylene is a nucleated and controlled rheology impact copolymer. 4944WZ is characterized by improved stiffness and impact resistance, as well as low shrinkage and low warpage. I.. |
|||
Melt Flow | 50 g/10 min @Load 10.0 kg, Temperature 220 °C |
50 g/10 min @Load 22.0 lb, Temperature 428 °F |
ASTM D 1238 |
Cossa Polimeri ESTADIENE 1030 V0/F Flame Retardant ABS Acrylonitrile Butadiene StyreneFlame retardant class V0, PBDE free, high melt flow rate, good impact resistance, high gloss, good light resistance, excellent processabilityInformation provided by Co.. |
|||
Melt Flow | 50 g/10 min @Load 2.16 kg, Temperature 190 °C |
50 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
ExxonMobil LL 6201.19 Injection Molding Resin Product Description: LL 6201 is a narrow molecular weight butane copolymer designed for applications that require excellent toughness. This resin offers easy processability for applications that req.. |
|||
Melt Flow | 50 g/10 min @Load 2.16 kg, Temperature 190 °C |
50 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
ExxonMobil LLDPE LL 6201RQ Molding Linear Low Density Polyethylene Resin (European Grade) Product Description: LL 6201 series are high flow LLDPE grades, which offer unique combination of excellent processability and outstanding product properties. Parts manufactured from LL 6201 Have go.. |
|||
Melt Flow | 50 g/10 min @Load 2.16 kg, Temperature 190 °C |
50 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238, ISO 1133 |
DuPont™ Elvaloy® AC 15024S Ethylene Methyl Acrylate Elvaloy® AC 15024S is a copolymer of ethylene and methyl acrylate. It is available in pellet form for use in conventional extrusion equipment designed to process polyethylene type resins. Elvaloy®.. |
|||
Melt Flow | 50 g/10 min @Load 5.00 kg, Temperature 275 °C |
50 g/10 min @Load 11.0 lb, Temperature 527 °F |
ISO 1133 |
Azoty Tarnow™ Tarnamid® T-29 MS Polyamide 6 - Natural Medium-high viscosity extrusion grade for mono or multilayer blown film, including biaxial oriented films, also for production of monofilament; can be used for injection molding and compounding.For .. |
|||
Melt Flow | 50 g/10 min @Load 5.00 kg, Temperature 275 °C |
50 g/10 min @Load 11.0 lb, Temperature 527 °F |
ISO 1133 |
Azoty Tarnow™ Tarnamid® T-29 Polyamide 6 - Natural Medium-high viscosity extrusion grade for mono or multilayer blown film, including biaxial oriented films, also for production of monofilament; can be used for injection molding and compounding.Tarn.. |
|||
Melt Flow | 50 g/10 min @Load 5.00 kg, Temperature 300 °C |
50 g/10 min @Load 11.0 lb, Temperature 572 °F |
ASTM D1238 |
BLUESTAR LXS 110 PPE-PS Typical Applications: Electrical partsFire RatedInformation provided by Polymer Technology and Services, LLC (PTS). |
|||
Melt Flow | 50 g/10 min @Load 5.00 kg, Temperature 275 °C |
50 g/10 min @Load 11.0 lb, Temperature 527 °F |
ISO 1133 |
Azoty Tarnow™ Tarnamid® T-27 GF30 Polyamide 6 - Glass Fiber Reinforced 30% Glass fiber reinforced, medium viscosity injection molding grade, also used for compounding, for production of monofilament, bristles and fibers.Tarnamid® has the following main properties:High.. |
|||
Melt Flow | 50 g/10 min @Load 5.00 kg, Temperature 235 °C |
50 g/10 min @Load 11.0 lb, Temperature 455 °F |
3 min; ASTM D1238 |
ALM PA 606-FR Filled Nylon 12 Prototyping Polymer Only commercially available fire retardant nylon 12 material, which meets FAR 25.853 60 second burn specification.The parts produced from PA 606-FR have a much smoother surface finish and sharper fe.. |
|||
Melt Flow | 50 g/10 min @Load 5.00 kg, Temperature 235 °C |
50 g/10 min @Load 11.0 lb, Temperature 455 °F |
3 min; ASTM D1238 |
ALM PA 614-GS Filled Nylon 12 Prototyping Polymer 40% glass sphere filled material for improved dimensional stability, increased stiffness, and higher temperature applications when compared to unfilled PA.Drop-in replacement for other commercially .. |
|||
Melt Flow | 50 g/10 min @Load 5.00 kg, Temperature 235 °C |
50 g/10 min @Load 11.0 lb, Temperature 455 °F |
3 min; ASTM D1238 |
ALM PA-615-GS Filled Nylon 12 Prototyping Polymer 50% glass sphere filled material for improved dimensional stability, increased stiffness, and higher temperature applications when compared to unfilled PA.Drop-in replacement for other commercially .. |
|||
Melt Flow | 50 g/10 min @Load 2.16 kg, Temperature 190 °C |
50 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
Bapolene® 3295 Polyethylene, Injection Grade Designed to offer improved cycle times and dimensional stability This product complies with US FDA 21CFR177.1250.Applications: Food containers and closures.Bapolene® and Bapolan® are registered t.. |
|||
Melt Flow | 50 g/10 min @Load 2.16 kg, Temperature 250 °C |
50 g/10 min @Load 4.76 lb, Temperature 482 °F |
ISO 1133 |
DuPont Performance Polymers Crastin® CE2055 BK580 PBT
(Unverified Data**) Crastin® CE2055 is an unreinforced, low viscosity polybutylene terephthalate resin for injection molding.Information provided by DuPont Performance Polymers |