Braskem H 203 HOMO Polypropylene Homopolymer

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene, Molded
Manufacturer Braskem
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Braskem H 203 HOMO Polypropylene Homopolymer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
H 203 is a high melt flow rate homopolymer with a general purpose additive package. This product exhibits excellent processability and good stiffness/impact strength balance. It also features a low taste/odor. It is designed for injection molding and fiber extrusion processing. Its applications include: injection of electric portables and household appliances; injected chest drawers and closets; continuous filaments for carpets, sewing threads, and ropes; staple fibers for rugs and blankets; and nonwovens by the thermobonded process.
Physical Properties Metric English Comments
Density 0.905 g/cc
0.0327 lb/in³
ASTM-D792
Melt Flow 20 g/10 min

@Load 2.16 kg,
Temperature 230 °C
20 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM-D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell R 97
97
ASTM-D785
Tensile Strength, Yield 35.0 MPa
5080 psi
ASTM-D638
Elongation at Yield 11 %
11 %
ASTM-D638
Flexural Modulus, 1% Secant 1100 MPa
160000 psi
ASTM-D790
Izod Impact, Notched 0.290 J/cm
0.543 ft-lb/in
ASTM-D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 96.0 °C
205 °F
ASTM-D648
Deflection Temperature at 1.8 MPa (264 psi) 56.0 °C
133 °F
ASTM-D648
Vicat Softening Point 152 °C

@Load 1.02 kg
306 °F

@Load 2.25 lb
ASTM-D1525