Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Braskem FF080WP Homopolymer Polypropylene

Category Polymer , Thermoplastic , Polypropylene (PP)
Manufacturer Braskem
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Braskem FF080WP Homopolymer Polypropylene.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: Superior Color and Processing Stability, Low Odor, Excellent Clarity, Excellent Slip PropertiesApplications: Suggested Uses include Cast FilmThis resin meets the requirements for olefin polymers as defined in 21 CFR, section 177.1520 issued by the Food and Drug Administration. The additives present are covered in appropriate regulation by FDA.Information provided by Braskem
Physical Properties Metric English Comments
Melt Flow 9.0 g/10 min

@Load 2.16 kg,
Temperature 230 °C
9.0 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength 36.2 MPa
5250 psi
2 in/min; ASTM D638
Elongation at Yield 13 %
13 %
2 in/min; ASTM D638
Flexural Modulus 1.38 GPa
200 ksi
0.05 in/min, 1% secant; ASTM D-790A
Izod Impact, Notched 0.267 J/cm
0.500 ft-lb/in
ASTM D256A
Users viewing this material also viewed the following: