Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength | 36.2 MPa | 5250 psi | 2 in/min; ASTM D638 |
Braskem FF080WP Homopolymer Polypropylene Description: Superior Color and Processing Stability, Low Odor, Excellent Clarity, Excellent Slip PropertiesApplications: Suggested Uses include Cast FilmThis resin meets the requirements for olefin.. |