Material Notes:
Description: General PurposeApplications: Suggested Uses Include Strapping, ProfilesThis resin meets the requirements for olefin polymers as defined in 21 CFR, section 177.1520 issued by the Food and Drug Administration. The additives present are covered in appropriate regulation by FDAInformation provided by Braskem
Physical Properties Metric English Comments
Melt Flow 1.3 g/10 min

@Load 2.16 kg,
Temperature 230 °C
1.3 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell R 101
101
ASTM D785
Tensile Strength 33.1 MPa
4800 psi
2 in/min; ASTM D638
Elongation at Yield 11 %
11 %
2 in/min; ASTM D638
Flexural Modulus 1.28 GPa
185 ksi
0.05 in/min, 1% secant; ASTM D-790A
Izod Impact, Notched 0.267 J/cm
0.500 ft-lb/in
ASTM D256A