Polymer Property : Tensile Strength = 4800 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength 33.1 MPa
4800 psi
ASTM D638
Quadrant EPP Proteus® O & P Grade, Natural Homopolymer Polypropylene (ASTM Product Data Sheet)
Tensile Strength 33.1 MPa
4800 psi
ASTM D638
Quadrant EPP Proteus® PP, Black Homopolymer Polypropylene (ASTM Product Data Sheet)
High impact resistance strength Better resistance to cracking at low temperatures than Homopolymer Polypropylene More pliable than homopolymer Meets food handling guidelines Chemical- and corrosion..
Tensile Strength 33.1 MPa
4800 psi
ASTM D638
Quadrant EPP Proteus® PP, Natural Homopolymer Polypropylene (ASTM Product Data Sheet)
Tensile Strength 33.1 MPa
4800 psi
ASTM D638
Quadrant EPP TIVAR® 88 ESD UHMW-PE, Premium Glass Filled, Crosslinked Electro Static Dissipative Lining Material (ASTM Product Data Sheet)
Tensile Strength 33.1 MPa
4800 psi
ASTM D638
Quadrant EPP TIVAR® 88-2 ESD Black, Premium Lubricant Filled, Lower COF, Electro Static Dissipative Lining Material (ASTM Product Data Sheet)
Tensile Strength 33.1 MPa
4800 psi
ASTM D638
Quadrant EPP Proteus® PP, ProKnob Finish Natural Homopolymer Polypropylene (ASTM Product Data Sheet)
High impact resistance strength Better resistance to cracking at low temperatures than Homopolymer Polypropylene More pliable than homopolymer Meets food handling guidelines Chemical- and corrosion..
Tensile Strength 33.1 MPa
4800 psi
ASTM D638
Ensinger Tecatron® XP-68 Compression Molded PPS Compound, 25% Fiberglass with Graphite
Ensinger Special Polymers has over twenty different grades of TECATRON PPS available. Custom formulations can be blended to suit specific applications. Compression molding is amenable to short run p..
Tensile Strength 33.1 MPa
4800 psi
2 in/min; ASTM D638
Braskem FPT300F Homopolymer Polypropylene
Description: Good mold release, excellent part finish (low bloom).Applications: Suggested uses include housewares, caps and closures, mugs / cups, thin-walled containers.Process: Injection Molding.T..
Tensile Strength 33.1 MPa
4800 psi
Product Property; Arlon SQA-TMS-048
Arlon T4015-R004 0.015" (0.381 mm) Thick, 1" wide, Cured Fusible Silicone Rubber with Sinusoidal Fiberglass Substrate
Design/Construction: Side 1: Cured Fusible Silicone RubberSubstrate: 15% Sinusoidal FiberglassSide 2: Cured Fusible Silicone Rubber Interleave: Polyester FilmArlon MOX-Tape® Fiberglass Reinforced T..
Tensile Strength 33.1 MPa
4800 psi
ASTM D638
Americas Styrenics STYRON® 404 High Impact Polystyrene
Product CharacteristicsAdditive FreeTypical ApplicationsCompounding and masterbatchesInformation provided by AmericasStyrenics LLC.
Tensile Strength 33.1 - 46.9 MPa
4800 - 6800 psi
Bulk Molding Compounds BMC A30 General Purpose Molding Compound
BMC A30 is a general purpose molding compound with good dimensional stability. Due to the excellent flow and controlled reactivity, BMC A30 is well suited for injection, transfer or compression mol..
Tensile Strength 33.1 - 46.9 MPa
4800 - 6800 psi
Bulk Molding Compounds BMC A30-3021 General Purpose Molding Compound
BMC A30-3021 is a low shrink, general purpose molding compound formulated for the lighting industry. A30-3021 is temperature stabilized for use in elevated temp. lighting applications. Due to the ..
Tensile Strength 33.1 MPa
4800 psi
ASTM D638
Aaron Industries AAROPRENE® TFPP 2030 Talc Filled Polypropylene
AAROPRENE® TFPP 2000 Series Talc Reinforced CompoundsMelt flow index may be specified. Color may be specified.
Tensile Strength 33.1 MPa
4800 psi
ASTM D638
Quadrant EPP Proteus® White Homopolymer Polypropylene (ASTM Product Data Sheet)
Tensile Strength 33.1 MPa
4800 psi
2 in/min; ASTM D638
Braskem F013M Homopolymer Polypropylene
Description: General PurposeApplications: Suggested Uses Include Strapping, ProfilesThis resin meets the requirements for olefin polymers as defined in 21 CFR, section 177.1520 issued by the Food an..