Borealis Bormed™ BE860MO Polypropylene Copolymer for Healthcare Applications

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene Copolymer
Manufacturer Borealis
Trade Name Bormed™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Borealis Bormed™ BE860MO Polypropylene Copolymer for Healthcare Applications.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Bormed BE860MO is a heterophasic copolymer characterized by an excellent impact strength also at low temperatures (deep freeze applications) together with high stiffness and good flow properties.Bormed BE860MO is designed for caps and closures, pharmaceutical and diagnostics packaging, and medical devices.Information provided by the Manufacturer.
Physical Properties Metric English Comments
Density 0.902 g/cc
0.0326 lb/in³
ISO 1183
Melt Flow 13 g/10 min

@Load 2.16 kg,
Temperature 230 °C
13 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ISO 1133
Mechanical Properties Metric English Comments
Hardness, Rockwell R 86
86
ISO 2039-2
Tensile Strength, Yield 25.0 MPa
3630 psi
At 50 mm/min; ISO 527-2
Elongation at Yield 6.0 %
6.0 %
At 50 mm/min; ISO 527-2
Tensile Modulus 1.25 GPa
181 ksi
At 1 mm/min; ISO 527-2
Charpy Impact, Notched 0.800 J/cm²
3.81 ft-lb/in²
ISO 179/1eA
0.400 J/cm²

@Temperature -20.0 °C
1.90 ft-lb/in²

@Temperature -4.00 °F
ISO 179/1eA
Impact Test 25.0 J

@Temperature -20.0 °C
18.4 ft-lb

@Temperature -4.00 °F
Instrumental Falling Weight - Total Penetration Energy; ISO 6603-2
35.0 J

@Temperature 0.000 °C
25.8 ft-lb

@Temperature 32.0 °F
Instrumental Falling Weight - Total Penetration Energy; ISO 6603-2
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 85.0 °C
185 °F
ISO 75-2