Beijing Evergrow Resources PTFE Gasket

Category Polymer , Thermoplastic , Fluoropolymer , PTFE , Polytetrafluoroethylene (PTFE), Molded
Manufacturer Beijing Evergrow Resources
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Beijing Evergrow Resources PTFE Gasket.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
PTFE gasket is manufactured by molding method with PTFE granular resin. PTFE compared with other plastics, has a superior properties against chemicals and temperature. Because of such excellent properties, PTFE has a wide application as a sealing material.Information provided by Beijing Evergrow Resources.
Physical Properties Metric English Comments
Density 2.10 - 2.30 g/cc
0.0759 - 0.0831 lb/in³
Mechanical Properties Metric English Comments
Tensile Strength at Break >= 15.0 MPa
>= 2180 psi
Elongation at Break >= 150 %
>= 150 %