Barlog Plastics KEBAFORM C 6027 POM Copolymer, 30% mineral reinforced

Category Polymer , Thermoplastic , Acetal (POM) , Acetal Copolymer, Mineral Filled
Manufacturer Barlog Plastics
Trade Name KEBAFORM
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Barlog Plastics KEBAFORM C 6027 POM Copolymer, 30% mineral reinforced.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
POM-MD30Information provided by BARLOG plastics GmbH.
Physical Properties Metric English Comments
Density 1.55 g/cc
0.0560 lb/in³
ISO 1183
Melt Flow 20 g/10 min

@Load 2.16 kg,
Temperature 190 °C
20 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ISO 1133
Mechanical Properties Metric English Comments
Tensile Strength at Break 60.0 MPa
8700 psi
ISO 527-1
Elongation at Break 8.0 %
8.0 %
ISO 527-1
Tensile Modulus 5.10 GPa
740 ksi
ISO 527-1
Charpy Impact Unnotched 5.50 J/cm²
26.2 ft-lb/in²
ISO 179-1eU
Charpy Impact, Notched 0.400 J/cm²
1.90 ft-lb/in²
ISO 179-1eA
Thermal Properties Metric English Comments
Melting Point 166 °C
331 °F
10°C/min; ISO 11357-1/-3
Deflection Temperature at 1.8 MPa (264 psi) 140 °C
284 °F
ISO 75-1/-2
Descriptive Properties Value Comments
Resin Type POM-MD30