Material Notes:
35 Durometer, 2-part, 10 to 1 mix, translucent, Fabric Coating grade, Liquid Silicone RubberInformation provided by Dow Corning
Physical Properties Metric English Comments
Specific Gravity 1.07 g/cc

@Temperature 25.0 °C
1.07 g/cc

@Temperature 77.0 °F
Solids Content 100 %
100 %
Viscosity 15000 cP
15000 cP
dynamic
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 4.41 MPa
640 psi
Elongation at Break 340 %
340 %
Tear Strength 5.08 kN/m
29.0 pli
Electrical Properties Metric English Comments
Volume Resistivity 4.80e+15 ohm-cm
4.80e+15 ohm-cm
Processing Properties Metric English Comments
Pot Life 4320 min
4320 min
Shelf Life 15.0 Month
15.0 Month
Descriptive Properties Value Comments
Appearance translucent
Gel Hardness (Grams/Penetration) 37
Mix Ratio (X:1) 10
Base to Catalyst