Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Bapolene® 3272 Polyethylene, Injection Grade

Category Polymer , Thermoplastic , Polyethylene (PE) , HDPE
Manufacturer Bapolene®
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Bapolene® 3272 Polyethylene, Injection Grade.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Narrow molecular weight distribution injection molding resin. This high flow resin allows fast injection cycles and provides good impact strength, rigidity, and warpage resistance. This product meets FDA standards for food contact applications.Applications: Thin-walled containers, housewares, and toys.Bapolene® and Bapolan® are registered trademarks of Bamberger Polymers, Inc. Information provided by Bamberger Polymers
Physical Properties Metric English Comments
Density 0.954 g/cc
0.0345 lb/in³
ASTM D1505
Melt Flow 20 g/10 min

@Load 2.16 kg,
Temperature 190 °C
20 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 24.8 MPa
3600 psi
2 in/min (50 mm/min); ASTM D638
Elongation at Break 350 %
350 %
2 in/min (50 mm/min); ASTM D638
Flexural Modulus 1.31 GPa
190 ksi
Tangent Method 1; ASTM D-790
Izod Impact, Notched 0.430 J/cm
0.806 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 80.0 °C
176 °F
ASTM D648
Vicat Softening Point 123 °C
253 °F
ASTM D1525
Descriptive Properties Value Comments
Process Injection Molding
Region Europe/Turkey
Bamberger Polymers Distribution
International
Bamberger Polymers Distribution
Mexico
Bamberger Polymers Distribution
US & Canada
Bamberger Polymers Distribution
Users viewing this material also viewed the following: