Bapolene 142B is a hexene linear low density polyethylene for blown film applications requiring superior impact strength. Product is designed to exhibit performance similar to that of super hexene products. It complies with US FDA 21CFR177.1520.Applications: General purpose, trash bags, and liners.Bapolene® and Bapolan® are registered trademarks of Bamberger Polymers, Inc. Information provided by Bamberger Polymers
Physical Properties Metric English Comments
Density 0.917 g/cc
0.0331 lb/in³
ASTM D-1505
Thickness 25.4 microns
1.00 mil
2.5:1 BUR as tested
Melt Flow 1.0 g/10 min

@Load 2.16 kg,
Temperature 190 °C
1.0 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Mechanical Properties Metric English Comments
Film Elongation at Break, MD 500 %
500 %
ASTM D-882
Film Elongation at Break, TD 650 %
650 %
ASTM D-882
Elmendorf Tear Strength MD 375 g
375 g
ASTM D-1922
Elmendorf Tear Strength TD 600 g
600 g
ASTM D-1922
Elmendorf Tear Strength, MD 14.8 g/micron
375 g/mil
ASTM D-1922
Elmendorf Tear Strength, TD 23.6 g/micron
600 g/mil
ASTM D-1922
Dart Drop Test 400 g
0.882 lb
F<sub>50</sub>; ASTM D-1709
Film Tensile Strength at Break, MD 37.0 MPa
5370 psi
ASTM D-882
Film Tensile Strength at Break, TD 27.0 MPa
3920 psi
ASTM D-882
Descriptive Properties Value Comments
Process Blown Film
Film
Region Europe/Turkey
Bamberger Polymers Distribution
International
Bamberger Polymers Distribution
Mexico
Bamberger Polymers Distribution
US & Canada
Bamberger Polymers Distribution
Users viewing this material also viewed the following:
Copyright © lookpolymers.com All Rights Reserved