Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Elmendorf Tear Strength TD | 600 g | 600 g | ASTM D1922 |
Iran Petrochemical (PCC) 235F7 Linear Low Density Polyethylene 235F7 is a LLDPE blown film grade designed for general purpose film application. This resin is particularly suited for blending with LDPE, giving better strength and downgauging possibility.Informat.. |
|||
Elmendorf Tear Strength TD | 600 g | 600 g | ASTM D1922 |
Westlake Mxsten CV77529 Polyethylene Plastomer Mxsten CV plastomer CV77529 is a polyethylene plastomer designed for blown film extrusion that contains high slip, very high antiblock and polymer processing aid additives. Films produced with this .. |
|||
Elmendorf Tear Strength TD | 600 g | 600 g | |
Dow DOWLEX™ 2045 Linear Low Density Polyethylene, Heavy Duty Film Grade DOWLEX® 2045 Polyethylene resin is a premier film resin for heavy duty applications. It complies with U.S. FDA regulation 21 CFR 177.1520 (c) 3.2(a) for food contact applications. The regulation sh.. |
|||
Elmendorf Tear Strength TD | 600 g | 600 g | |
Dow DOWLEX™ 2045A Linear Low Density Polyethylene, Blown Film Grade DOWLEX® 2045A Polyethylene blown film extrusion resin is a premier film resin for heavy duty applications. It is utilized where improved thermal stability over a broader range of processing conditi.. |
|||
Elmendorf Tear Strength TD | 600 g | 600 g | |
Dow DOWLEX™ 2056 Linear Low Density Polyethylene, Heavy Duty Film Grade DOWLEX® 2056 Polyethylene resin is a premier polymer for heavy duty blown film applications. It is a low gel, high consistency polymer. It complies with U.S. FDA Regulation 21 CFR 177.1520 (c) 3.2 .. |
|||
Elmendorf Tear Strength TD | 600 g | 600 g | |
Dow DOWLEX™ 2056A Linear Low Density Polyethylene, Heavy Duty Film Grade DOWLEX® 2056A Polyethylene is a premier polymer for heavy duty blown film applications. It is a low gel, high consistency polymer with improved thermal stability and is an outstanding choice for cr.. |
|||
Elmendorf Tear Strength TD | 600 g | 600 g | |
Dow DOWLEX™ 2101 Linear Low Density Polyethylene, Blown Film Grade DOWLEX® 2101 Polyethylene resin, a general purpose blown film extrusion resin, is an excellent choice for high speed, thin gauge film applications. It contains medium levels of both slip additive a.. |
|||
Elmendorf Tear Strength TD | 600 g | 600 g | |
Dow DOWLEX™ 2245A Linear Low Density Polyethylene, Heavy Duty Film Grade DOWLEX® 2245A Polyethylene resin is a premier film resin for heavy duty applications. DOWLEX 2245A resin is used where improved thermal stability over a broad range of processing conditions is nece.. |
|||
Elmendorf Tear Strength TD | 600 g | 600 g | |
Dow DOWLEX™ 2245D Linear Low Density Polyethylene, Heavy Duty Film Grade DOWLEX® 2245D Polyethylene resin is a premier film resin for heavy duty applications. DOWLEX 2245D resin is used where improved thermal stability over a broad range of processing conditions is nece.. |
|||
Elmendorf Tear Strength TD | 600 g | 600 g | ASTM D1922 |
Dow ELITE™ 5220G Enhanced Polyethylene Resin High impact and puncture resistance Excellent on-pallet load elongation for higher yields on regular loads Complies with U.S. FDA 21 CFR 177.1520 (c) 3.2a Information provided by Dow |
|||
Elmendorf Tear Strength TD | 600 g | 600 g | ASTM D-1922 |
Bapolene® 142A Polyethylene Film Grade Bapolene 142A is a hexene linear low density polyethylene for blown film applications requiring superior impact strength. Product is designed to exhibit performance similar to that of super hexene p.. |
|||
Elmendorf Tear Strength TD | 600 g | 600 g | ASTM D-1922 |
Bapolene® 142B Polyethylene Film Grade Bapolene 142B is a hexene linear low density polyethylene for blown film applications requiring superior impact strength. Product is designed to exhibit performance similar to that of super hexene p.. |
|||
Elmendorf Tear Strength TD | 600 g | 600 g | ASTM D-1922 |
Bapolene® 142F Polyethylene Film Grade Bapolene 142F is a hexene linear low density polyethylene for blown film applications requiring superior impact strength. Product is designed to exhibit performance similar to that of super hexene p.. |
|||
Elmendorf Tear Strength TD | 600 g | 600 g | ASTM D-1922 |
Bapolene® 152A Polyethylene Film Grade Bapolene 152A is a hexene linear low density polyethylene with a combination of superior impact strength and HSIT. Product is designed to exhibit performance similar to that of metallocene products... |
|||
Elmendorf Tear Strength TD | 600 g | 600 g | ASTM D-1922 |
Bapolene® 152B Polyethylene Film Grade Bapolene 152B is a hexene linear low density polyethylene with a combination of superior impact strength and HSIT. Product is designed to exhibit performance similar to that of metallocene products... |
|||
Elmendorf Tear Strength TD | 600 g | 600 g | ASTM D-1922 |
Bapolene® 152F Polyethylene Film Grade Bapolene 152F is a hexene linear low density polyethylene with a combination of superior impact strength and HSIT. Product is designed to exhibit performance similar to that of metallocene products... |
|||
Elmendorf Tear Strength TD | 600 g | 600 g | |
Westlake Hifor SC74560-F Clear Polyethylene
(discontinued **) Hifor Clear Polyethylene SC74560-F polymer is a high strength and high clarity polyethylene designed for blown film extrusion that contains medium slip and medium antiblock additives. Films produc.. |
|||
Elmendorf Tear Strength TD | 600 g | 600 g | ASTM D1922 |
M. Holland Company MAGMA® LM115-C LLDPE
(discontinued **) Additives: Medium Antiblock, Low SlipFeatures: Good Processability, Good Puncture Resistance, Good Tear Strength, Good ToughnessProcessing Method: ExtrusionInformation provided by M. Holland. |