Material Notes:
Description: Polyoxymethylene based batch with approx. 20% carbon black for coloring thermoplastic polyoxymethylenes. Recommended concentrations of FK61002 batch within the mixture with thermoplastic polyoxymethylenes are in the range of 1 to 2 %. Higher concentrations (up to 10 %) may yield further improved UV stability but will reduce toughness.Information provided by BASF
Physical Properties Metric English Comments
Bulk Density 0.890 g/cc
0.0322 lb/in³
Density 1.40 g/cc
0.0506 lb/in³
DIN 53479
Melt Flow 35 g/10 min

@Load 10.0 kg,
Temperature 190 °C
35 g/10 min

@Load 22.0 lb,
Temperature 374 °F
ISO 1133
Thermal Properties Metric English Comments
Melting Point 165 °C
329 °F
ISO 11357-1/-3
Decomposition Temperature >= 240 °C
>= 464 °F
Processing Properties Metric English Comments
Melt Temperature 190 - 230 °C
374 - 446 °F
Injection molding
Descriptive Properties Value Comments
Color Black
Commercial Status Europe
Ignition Temperature 320 - 340 °C
ASTM D1929