Thermal Properties | Metric | English | Comments |
---|---|---|---|
Decomposition Temperature | 240 - 280 °C | 464 - 536 °F | |
Oceanchem Group Tris (chloroethyl) Phosphate (TCEP) Molecular Formula: C6H12O4Cl3PCas No.: 29716-44-7Property: It is colorless or light yellow oily transparent liquid with slight cream odor. Soluble in common organic solvents, insoluble in aliphatic.. |
|||
Decomposition Temperature | >= 240 °C | >= 464 °F | Thermal Stability; ASTM D2513/D3350 |
Ineos TUB 121NTW HDPE TUB121 NTW is a natural high density bimodal polyethylene copolymer designed for extrusion of large diameter, thick wall piping for potable water, industrial and mining applications. When blended wi.. |
|||
Decomposition Temperature | >= 240 °C | >= 464 °F | |
BASF Ultraform® E 3120 BM POM Description: Is a POM, high-molecular grade for extrusion blow molding of hollow parts.Information provided by BASF |
|||
Decomposition Temperature | >= 240 °C | >= 464 °F | |
BASF Ultraform® FK 61002 20% Carbon Black Filled POM Description: Polyoxymethylene based batch with approx. 20% carbon black for coloring thermoplastic polyoxymethylenes. Recommended concentrations of FK61002 batch within the mixture with thermoplasti.. |
|||
Decomposition Temperature | >= 240 °C | >= 464 °F | |
BASF Ultraform® H2320 004 POM Description: Is a POM, high-molecular-weight grade for extrusion of small thin-walled pipes and panel.Information provided by BASF |
|||
Decomposition Temperature | >= 240 °C | >= 464 °F | |
BASF Ultraform® N2520 L POM Description: Is a POM, product having reduced electric surface resistance.Information provided by BASF |
|||
Decomposition Temperature | >= 240 °C | >= 464 °F | |
BASF Ultraform® N2640 E2 POM Description: Is a POM + MBS, elastomer-modified injection-molding grade with enhanced toughness and high weld line strength.Information provided by BASF |
|||
Decomposition Temperature | >= 240 °C | >= 464 °F | |
BASF Ultraform® N2640 E4 POM Description: Is a POM + MBS, elastomer-modified injection-molding grade with high toughness and high weld line strength.Information provided by BASF |
|||
Decomposition Temperature | >= 240 °C | >= 464 °F | |
BASF Ultraform® N2640 Z2 POM + PUR Description: Elastomer-modified injection molding grade with high impact strength for clips, snap and fastening elements, and also for components subject to impact stress.Information provided by BAS.. |
|||
Decomposition Temperature | >= 240 °C | >= 464 °F | |
BASF Ultraform® N2650 Z4 POM + PUR Description: Elastomer-modified injection molding grade with high impact strength for clips, snap and fastening elements, and also for components subject to impact stress.Information provided by BAS.. |
|||
Decomposition Temperature | >= 240 °C | >= 464 °F | |
BASF Ultraform® N2720 M210 POM Description: Is a POM, product with increased stiffness and strength as well as good wear characteristics, used, for instance, for sliding chains and conveyor systems.Information provided by BASF |
|||
Decomposition Temperature | >= 240 °C | >= 464 °F | |
BASF Ultraform® N2770 K POM Description: Is a POM, injection-molding grade with improved wear characteristics for sliding elements.Information provided by BASF |
|||
Decomposition Temperature | >= 240 °C | >= 464 °F | |
BASF Ultraform® S2320 0035 LEV POM Description: Is a POM, free-flowing and rapidly solidifying standard grade with reduced emission potential for injection molding.Information provided by BASF |
|||
Decomposition Temperature | >= 240 °C | >= 464 °F | |
BASF Ultraform® W2320 003 PRO POM Description: Is a POM, is a very easy flowing grade for thin-walled components with long flow paths.Information provided by BASF |
|||
Decomposition Temperature | >= 240 °C | >= 464 °F | |
BASF Ultraform® W2320 U03 POM Description: Very free-flowing, rapidly solidifying grade with UV stabilization for use where processing is extremely difficult but mechanical requirements are lower.Information provided by BASF |
|||
Decomposition Temperature | >= 240 °C | >= 464 °F | |
BASF Ultraform® W2320 U035 LEV POM Description: Is a POM, UV-stabilized, very free-flowing, rapidly solidifying grade for injection molding, with reduced emission potential.Information provided by BASF |
|||
Decomposition Temperature | >= 240 °C | >= 464 °F | |
BASF Ultraform® Z2320 003 POM Description: Is a POM, rapidly solidifying grade for applications with exceptional demands on flowability.Information provided by BASF |
|||
Decomposition Temperature | >= 240 °C | >= 464 °F | |
BASF Ultraform® FK 66003 20% Silicone Filled POM Description: Polyoxymethylene based batch with approx. 20% silicone (polysiloxane) for modifying tribological properties of thermoplastic polyoxymethylenes. Recommended concentrations of batch FK660.. |
|||
Decomposition Temperature | >= 240 °C | >= 464 °F | |
BASF Ultraform® N2320 0035 POM Description: Rapidly solidifying standard grade for injection molding.Information provided by BASF |
|||
Decomposition Temperature | >= 240 °C | >= 464 °F | |
BASF Ultraform® N2720 M63 30% Mineral Filled POM Description: Is a POM, 30 % mineral-reinforced material for low-warpage moldings with high stiffness, strength and hardness.Information provided by BASF |
|||
Decomposition Temperature | >= 240 °C | >= 464 °F | |
BASF Ultraform® S2320 003 POM Description: Easy flowing and rapidly freezing grade for injection molding difficult, thin-walled part.Information provided by BASF |
|||
Decomposition Temperature | >= 240 °C | >= 464 °F | |
BASF Ultraform® S2320 003 PRO POM Description: Is a POM, is a standard flowing and rapidly freezing grade suitable for standard functional applications.Information provided by BASF |
|||
Decomposition Temperature | >= 240 °C | >= 464 °F | |
BASF Ultraform® W2320 0035 POM Description: Is a POM, very free-flowing and rapidly solidifying grade for high processing demands.Information provided by BASF |
|||
Decomposition Temperature | >= 240 °C | >= 464 °F | |
BASF Ultraform® N2520 XL2 POM Description: Is a POM, injection-molding grade with increased electrical conductivity, for applications with reduced mechanical requirements.Information provided by BASF |
|||
Decomposition Temperature | >= 240 °C | >= 464 °F | |
BASF Ultraform® N2650 Z6 POM + PUR Description: Elastomer-modified injection molding grade for applications requiring highest impact strength together with low stiffness.Information provided by BASF |
|||
Decomposition Temperature | >= 240 °C | >= 464 °F | |
BASF Ultraform® N2644 Z9 POM + PUR Description: Elastomer modified injection molding grade for applications requiring low modulus. Good acoustic damping.Information provided by BASF |