Material Notes:
Recommended use: For the production of homopolymerisates and copolymerisates, initial product for chemical synthesesInformation provided by BASF
Physical Properties Metric English Comments
Bulk Density 0.700 g/cc
0.0253 lb/in³
Density 1.36 g/cc
0.0491 lb/in³
Solubility in Water 2.3 %
2.3 %
pH 2.7
2.7
100 g/l
Molecular Weight 146.14 g/mol
146.14 g/mol
Vapor Pressure 0.0000970 bar

@Temperature 25.0 °C
0.0728 torr

@Temperature 77.0 °F
Thermal Properties Metric English Comments
Melting Point 150.85 °C
303.53 °F
Boiling Point 337.5 °C

@Pressure 0.1031 MPa
639.5 °F

@Pressure 14.96 psi
Flash Point >= 196 °C
>= 385 °F
Descriptive Properties Value Comments
Color White
Commercial Status Europe
Ignition Temperature 405°C
DIN 51794
Minimum Ignition energy 1 bar; VDI 2263, sheet 1, 2.5
Copyright © lookpolymers.com All Rights Reserved