Polymer Property : Melting Point = 150.85 °C
Polymer Property :
Melting Point =
150.85 °C
Product List
Thermal Properties
Tips:
30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties
Metric
English
Comments
Melting Point
150.85
°C
303.53
°F
BASF Adipic Acid
Recommended use: For the production of homopolymerisates and copolymerisates, initial product for chemical synthesesInformation provided by BASF