Physical Properties | Metric | English | Comments |
---|---|---|---|
Bulk Density | 0.700 g/cc | 0.0253 lb/in³ | Tapped |
Nyco ASPECT® 4000 Wollastonite ASPECT 4000 is available untreated or with a surface modification treatment.Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distinctive .. |
|||
Bulk Density | 0.700 g/cc | 0.0253 lb/in³ | Tapped |
Nyco M3 WOLLASTOCOAT® Wollastonite Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distinctive particle morphology makes wollastonite an ideal performance mineral for a br.. |
|||
Bulk Density | 0.700 - 0.900 g/cc | 0.0253 - 0.0325 lb/in³ | |
Nabaltec NABALOX® NO 115 TC Ground Alumina NABALOX® aluminum oxide has a number of advantages including low sintering temperaturewide sintering rangeflexible processinghigh sintered densities high wear and impact resistanceelectrical insula.. |
|||
Bulk Density | 0.700 - 0.900 g/cc | 0.0253 - 0.0325 lb/in³ | |
Nabaltec NABALOX® NO 115-71 Ground Alumina NABALOX® aluminum oxide has a number of advantages including low sintering temperaturewide sintering rangeflexible processinghigh sintered densities high wear and impact resistanceelectrical insula.. |
|||
Bulk Density | 0.700 - 0.900 g/cc | 0.0253 - 0.0325 lb/in³ | |
Nabaltec NABALOX® NO 615-10 Reactive Alumina NABALOX® aluminum oxide has a number of advantages including low sintering temperaturewide sintering rangeflexible processinghigh sintered densities high wear and impact resistanceelectrical insula.. |
|||
Bulk Density | 0.700 - 0.950 g/cc | 0.0253 - 0.0343 lb/in³ | |
Magyar Aluminum ALO-P54 Alumina Alumina for Polishing |
|||
Bulk Density | 0.700 g/cc | 0.0253 lb/in³ | ISO 60 |
Lanxess Durethan® AKV 30 000000 Nylon 66, Glass Fiber Reinforced PA 66, 30% glass fibers, injection moldingInformation provided by LANXESS. |
|||
Bulk Density | 0.700 g/cc | 0.0253 lb/in³ | ISO 60 |
Lanxess Durethan® B 31 FCS 000000 Nylon 6, Film Grade PA 6, non-reinforced, extrusion, low viscosity, slip agentInformation provided by LANXESS. |
|||
Bulk Density | 0.700 g/cc | 0.0253 lb/in³ | ISO 60 |
Lanxess Durethan® B 40 SK 000000 Nylon 6 PA 6, non-reinforced, injection molding |
|||
Bulk Density | 0.700 g/cc | 0.0253 lb/in³ | ISO 60 |
Lanxess Durethan® BG 30 X W1 000000 Nylon 6, Glass Fiber Reinforced PA 6, 30% glass fibers/glass spheres, injection molding, low tendency to warp, weather stabilizedInformation provided by LANXESS. |
|||
Bulk Density | 0.700 g/cc | 0.0253 lb/in³ | ISO 60 |
Lanxess Durethan® BKV 50 H2.0 EF DUS30 901510 Nylon 6, Glass Fiber Reinforced PA 6, 50% glass fibers, injection molding, improved flowability, heat-aging stabilizedInformation provided by LANXESS. |
|||
Bulk Density | 0.700 g/cc | 0.0253 lb/in³ | ISO 60 |
Lanxess Pocan® A 3121 901510 PBT+ASA, 20% Glass Fiber PBT + ASA, 20% glass fibers, injection molding, low tendency to warp, improved surface finishInformation provided by LANXESS. |
|||
Bulk Density | 0.700 g/cc | 0.0253 lb/in³ | ISO 60 |
Lanxess Pocan® BF 4130 XF 000000 PBT, 30% Glass Fiber PBT, 30% glass fibers, injection molding, flame retardant, improved flowabilityInformation provided by LANXESS. |
|||
Bulk Density | 0.700 g/cc | 0.0253 lb/in³ | Apparent Density |
Indium Corp. Ga2O3 Gallium Sesquioxide Synonyms: Gallium Oxide, Gallium (III) OxideCAS Number: 12024-21-4EC Number: 234-691-7RTECS: LW9650000Purity: 99.99 to 99.999% Gallium SesquioxideAppearance/Form: White powderCrystal structure.. |
|||
Bulk Density | 0.700 - 0.760 g/cc | 0.0253 - 0.0275 lb/in³ | After drying at 110°C |
Gouda Vuurvast GOLITE 95 Refractory Insulating Castable Description: Golite 95 is widely applied as an insulating backlining behind a dense castable, especially in the petrochemical industry.Remarks: These values apply to cast products. Also available in.. |
|||
Bulk Density | 0.700 g/cc | 0.0253 lb/in³ | ISO 60 |
Lanxess Pocan® TP 740-202 901510 PBT+ASA, 20% Glass Fiber PBT + ASA, 20% glass fibers, injection molding, low tendency to warp, improved surface finishInformation provided by LANXESS. |
|||
Bulk Density | 0.702 g/cc | 0.0253 lb/in³ | Dry |
Skamol Group SKAMOLEX V-1100 (700) Panel Design SKAMOLEX panel designs have the following characteristics: Max. service temperature: Up to 1150°C (2102°F)Hot-face applications or back-up insulationA large variety of specialized and versatil.. |
|||
Bulk Density | 0.700 g/cc | 0.0253 lb/in³ | |
Solvay JAGUAR® HP 8 COS Surfactant Description: Hydroxypropyl Guar for thickening, which provides a fluid and smooth wet feel to formulationsChemical Name: Guar Gum DerivativeC.T.F.A./I.N.C.I. Name: Hydroxypropyl GuarCAS: 39421-75-5S.. |
|||
Bulk Density | 0.700 g/cc | 0.0253 lb/in³ | ASTM D1895 |
Sumitomo Bakelite Sumikon® PM-6430 Glass-Filled Phenolic, Injection Grade Sumikon PM-6430 black Phenolic is a two stage glass fiber and mineral filled special purpose molding compound. It is especially designed for applications requiring high strength and dimensional s.. |
|||
Bulk Density | 0.700 g/cc | 0.0253 lb/in³ | ASTM D1895 |
Sumitomo Bakelite North America E 2748A Short Glass Fiber Reinforced Epoxy E 2748A is a glass reinforced epoxy molding compound, with good impact strength combined with soft flow for the encapsulation of devices requiring high quality and thermal shock resistance.Informati.. |
|||
Bulk Density | 0.700 - 0.800 g/cc | 0.0253 - 0.0289 lb/in³ | |
Solvay RHODICARE CFT Surfactant Description: Rhodicare® CFT is Cellulase-free clear grade of Xanthan Gum, it is recommended when associated with cellulose-based polymers. Approved for Ecocert. It is excellent anionic bio-polyme.. |
|||
Bulk Density | 0.700 - 0.800 g/cc | 0.0253 - 0.0289 lb/in³ | |
Solvay RHODICARE T Surfactant Description: Rhodicare® T is high purity grade specifically designed for thickening and suspension in clear formulations. It has high electrolyte stability over a wide range of pH and fast hydrat.. |
|||
Bulk Density | 0.700 - 0.800 g/cc | 0.0253 - 0.0289 lb/in³ | |
Solvay RHODOPOL® T Surfactant Description: Transparent grade xanthan gum. It is It exhibits high pseudoplastic behavior effective thickening and stabilizing agent.Identification: XANTHAN GUMCAS: 11138 – 66 – 2Available.. |
|||
Bulk Density | 0.700 - 0.850 g/cc | 0.0253 - 0.0307 lb/in³ | Powder Density; ISO 60 |
Vyncolit X681 Novolac Phenolic Glass fiber filled phenolic molding compound with excellent mechanical properties and a low coefficient of friction. Tribological compound with PTFE additive.USES: Water pump seals and self-lubrica.. |
|||
Bulk Density | 0.700 g/cc | 0.0253 lb/in³ | Powder Density; ISO 60 |
Vyncolit G865 Novolac Phenolic Glass fiber filled phenolic molding compound with high mechanical, good thermal and electrical properties. USES: Asbestos-free replacement for die-cast automotive metal parts, e.g. reactors for aut.. |
|||
Bulk Density | 0.700 - 0.800 g/cc | 0.0253 - 0.0289 lb/in³ | |
BASF Ultrason® E 3010 MR UN PESU Description: Unreinforced, higher viscosity injection molding and extrusion grade with improved toughness and chemical resistance (stress crack resistance); demolding optimized. Abbreviated designat.. |
|||
Bulk Density | 0.700 - 0.800 g/cc | 0.0253 - 0.0289 lb/in³ | |
BASF Ultrason® E 2010 SW Q31 10088 PESU Information provided by BASF |
|||
Bulk Density | 0.700 - 0.800 g/cc | 0.0253 - 0.0289 lb/in³ | |
BASF Ultrason® KR 4113 PESU with 10/10% Carbon Fibers/Graphite and 10% PTFE Description: Compound based on PES with 30 % filler. The filler system, a mixture of carbon fibers, graphite and PTFE powder, considerably improves Ultrason’s tribological properties. In addition, .. |
|||
Bulk Density | 0.700 g/cc | 0.0253 lb/in³ | ASTM D1895 |
Sumitomo Bakelite Sumikon® PM-6430 Glass-Filled Phenolic, Compression Grade Sumikon PM-6430 black Phenolic is a two stage glass fiber and mineral filled special purpose molding compound. It is especially designed for applications requiring high strength and dimensional sta.. |