Thermal Properties Metric English Comments
Flash Point 196 °C
385 °F
LG Chemical DOA Plasticizer
Features: LG DOA is an aliphatic plasticizer and used to keep softness of product under cold water.Application: Wrap for food package, synthetic leather, sheet, hose, gasketInformation provided by L..
Flash Point 196 °C
385 °F
Lubriplate 68-N Naphthenic Refrigeration Compressor Oil
These highly refined lubricants are formulated for use in refrigeration compressor systems utilizing ammonia, CFC (chlorofluorocarbon) and HCFC (hydrochlorofluorocarbon) refrigerants such as R-717, ..
Flash Point 196 °C
385 °F
Heatbath/Park High Speed Vacuum Quench Oil
Faster quench speed than VQO above, but otherwise very similar. Information provided by Heatbath Corporation - Park Metallurgical.
Flash Point 196 °C
385 °F
open cup
Solvay Chemicals IXOL® B 251
IXOL® B 251 is also suitable for the development of formulations having high fire performance according to the new European standard based on the Single Burning Item (SBI) test. As example, formu..
Flash Point 196 °C
385 °F
The Chemical Company Adipic Acid, C6H10O4
Adipic Acid is a mildly toxic, white, crystalline compound. The C6 straight-chain dicarboxylic acid is slightly soluble in water and soluble in alcohol and acetone. Nearly all commercial Adipic Acid..
Flash Point 196 °C
385 °F
ASTM D92
ChevronTexaco MERCON® V Automatic Transmission Fluid
Beginning with the 1997 model year, Ford introduced a higher performance level ATF with the MERCON V specification. Many Ford automatic transmissions from 1999 on will require a MERCON V fluid. The ..
Flash Point 196 °C
385 °F
ASTM D92
ChevronTexaco Rykon® 5W-20 Premium Oil MV
FeaturesChevron Rykon Premium Oil MV is a versatile multiviscosity lubricant designed to give maximum protection to hydraulic pumps.It is formulated with ISOSYN® base stocks and contains a shear st..
Flash Point 196 °C
385 °F
See Note 3.
ChevronTexaco Thread Compound
Texaco Thread Compound delivers value through:Ability to meet API requirements for high-pressure thread compounds.Galling prevention — Prevents galling in threaded connections. Joints are easier to..
Flash Point 196 °C
385 °F
See Note 3.
ChevronTexaco Threadtex®
Texaco Threadtex delivers value through:High antiweld protection — Drill collars "break" easily. No galled or broken threads.Excellent lubrication in the presence of water, drilling muds, etc. Prov..
Flash Point 196 °C
385 °F
ConocoPhillips Hydroclear® 15 Rolling Oil
Description: Conoco Hydroclear Rolling Oil is a multipurpose rolling oil formulated from premium Conoco hydrocracked base stocks. Hydroclear Rolling Oil is specially formulated with proprietary addi..
Flash Point 196 °C
385 °F
ASTM D92
ChevronTexaco Bright-Cut® AXH Metal Working Fluid
FeaturesChevron Bright-Cut Metalworking Fluids are a complete line of chlorine-free cutting oils that offer benefits not found in conventional cutting oils.The unique synthetic antiweld components ..
Flash Point 196 °C
385 °F
ChevronTexaco Havoline® MERCON® V Automatic Transmission Fluid
Havoline Automatic Transmission Fluid MERCON V delivers value through:Protection against the formation of lacquers, sludge, or other harmful deposits.Exceptional stability provided by excellent base..
Flash Point 196 °C
385 °F
closed cup
Aquabond Technologies Aquabond™ ABS-55 Water Soluble Adhesive and Bonding Thermoplastic
Description: Aquabond's water soluble thermoplastic is designed for temporary mounting of hard materials for slicing, dicing, grinding, lapping and polishing and comes in 3 different bonding tem..
Flash Point 196 °C
385 °F
closed cup
Aquabond Technologies Aquabond™ ABS-65 Water Soluble Adhesive and Bonding Thermoplastic
Description: Aquabond's water soluble thermoplastic is designed for temporary mounting of hard materials for slicing, dicing, grinding, lapping and polishing and comes in 3 different bonding tem..
Flash Point 196 °C
385 °F
ConocoPhillips 22 Super Hydraulic Oil
Description: Conoco Super Hydraulic Oil is a high-quality antiwear hydraulic fluid formulated from premium Conoco hydrocracked base stocks to provide superior water separation, antiwear protection, ..
Flash Point >= 196 °C
>= 385 °F
BASF Adipic Acid
Recommended use: For the production of homopolymerisates and copolymerisates, initial product for chemical synthesesInformation provided by BASF