Azoty Tarnow™ Alphalon™ 25 Nylon 6

Category Polymer , Thermoplastic , Nylon , Nylon 6
Manufacturer Azoty Tarnow™ (Zaklady Azotowe)
Trade Name Alphalon™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Azoty Tarnow™ Alphalon™ 25 Nylon 6.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
A bright polyamide 6 grade of low viscosity suited for the production of compounds.Information provided by ATT Polymers™
Physical Properties Metric English Comments
Specific Gravity 1.13 g/cc
1.13 g/cc
ISO 1183
Relative Viscosity 2.45 - 2.55 cP
2.45 - 2.55 cP
1% in 96% H2SO4; ISO 307
Viscosity Test 132 cm³/g
132 cm³/g
0.5% in 96% H2SO4; ISO 307
Thermal Properties Metric English Comments
Melting Point 220 °C
428 °F
ISO 3146
Component Elements Properties Metric English Comments
TiO2 0.00 %
0.00 %
Processing Properties Metric English Comments
Moisture Content <= 0.10 %
<= 0.10 %
Brabender
Descriptive Properties Value Comments
Chip Shape cylindrical
Chip Size, mm 2.5
Extract Content, % internal