Physical Properties | Metric | English | Comments |
---|---|---|---|
Relative Viscosity | 2.45 - 2.55 cP | 2.45 - 2.55 cP | 1% in 96% H2SO4; ISO 307 |
Azoty Tarnow™ Alphalon™ 25 Nylon 6 A bright polyamide 6 grade of low viscosity suited for the production of compounds.Information provided by ATT Polymers™ |