Physical Properties | Metric | English | Comments |
---|---|---|---|
Particle Size | <= 3000 µm | <= 3000 µm | Grain Size |
Gouda Vuurvast CURON 160 HF Dense Refractory Castable Description: This castable has a high volume stability and keeps its strength up to high temperatures. In addition, Curon 160 HF has an excellent thermal shock resistance. It is largely used in the .. |
|||
Particle Size | <= 3000 µm | <= 3000 µm | Grain Size |
Gouda Vuurvast FLUCON 160 K Dense Self Flowing Refractory Castable Description: Flucon 160 K is a self-flowing low cement castable based on silicon carbide. This castable is characterized by high strength high abrasion resistance and excellent thermal shock resista.. |
|||
Particle Size | <= 3000 µm | <= 3000 µm | Grain Size |
Gouda Vuurvast GOLITE 160 Refractory Insulating Castable Description: This castable can be used up to very high temperatures under reducing conditions.Remarks: These values apply to cast products. Also available in gunning variety, marked "GM".Information.. |
|||
Particle Size | 3000 - 8000 µm | 3000 - 8000 µm | Lumpy |
H.C. Starck Grade K2 Crystalline Boron Neutron shields and absorbers in nuclear reactorsThermistorsFilamentsPreparation of high-purity metal boridesMetallurgy (deoxidizing agent) |
|||
Particle Size | <= 3000 µm | <= 3000 µm | Grain Size |
Gouda Vuurvast VIBRON 162 K Sp Dense Vibrating Refractory Silicon Carbide Castable Vibron 162 K Sp is a low cement castable based on silicon carbide. This castable is characterized by a very good thermal conductivity, a high abrasion resistance and high resistance against oxidatio.. |
|||
Particle Size | 3000 µm | 3000 µm | Flat Cylinder Shape; DAK-QAR-SOP-0017 |
DAK Americas Laser+® B90B PET Product Description: Laser+® (B90B) polyethylene terephthalate (PET) resin is a copolymer formulated for conversion to PET bottles by conventional single or two-stage processing technology.Typical .. |
|||
Particle Size | 3000 µm | 3000 µm | Flat Cylinder Shape; DAK-QAR-SOP-0017 |
DAK Americas Laser+® C (C60A) PET Product Description: Laser+® C (C60A) is a unique copolymer particularly suited for use in the custom PET container applications where clarity and neutral colored are desired. It is a medium intrin.. |
|||
Particle Size | 3000 µm | 3000 µm | Flat Cylinder Shape; DAK-QAR-SOP-0017 |
DAK Americas Laser+® C (E60A) PET Product Description: Laser+® C (E60A) is a unique copolymer particularly suited for use in the custom PET container applications where clarity and neutral colored are desired. It is a medium intrin.. |
|||
Particle Size | 3000 µm | 3000 µm | Flat Cylinder Shape; DAK-QAR-SOP-0017 |
DAK Americas Laser+® HS D59A PET Product Description: Laser+® HS (D59A) polyethylene terephthalate (PET) resin is designed for conversion to PET packaging by injection stretch blow-molding using commercial heat-set technology.Typi.. |
|||
Particle Size | 3000 µm | 3000 µm | Flat Cylinder Shape; DAK-QAR-SOP-0017 |
DAK Americas Laser+® W L44A PET Product Description: Laser+® W (L44A) polyethylene terephthalate (PET) resin is a copolymer formulated for conversion to PET bottles by conventional single or two-stage processing technology.Typica.. |
|||
Particle Size | 3000 µm | 3000 µm | Flat Cylinder Shape; DAK-QAR-SOP-0017 |
DAK Americas Laser+® W L44B PET Product Description: Laser+® W (L44A) polyethylene terephthalate (PET) resin is a copolymer formulated for conversion to PET bottles by conventional single or two-stage processing technology.Typica.. |
|||
Particle Size | 3000 µm | 3000 µm | Spherical Shape; DAK-QAR-SOP-0017 |
DAK Americas Laser+® W P41A PET Product Description: Laser+® W (P41A) polyethylene terephthalate (PET) resin is a copolymer formulated for conversion to PET bottles by conventional single or two-stage processing technology.Typica.. |
|||
Particle Size | 3000 µm | 3000 µm | Pellet Size |
Axion Polymers Axpoly® HDPE21 1000 High Purity Molding Produced from 100% post-consumer raw materials, this product fits closely with Axion's other recycled resin grades and offers the same set of user benefits, including:Successfully replaces virgin re.. |
|||
Particle Size | 3000 µm | 3000 µm | Typical |
Axion Polymers Axpoly® PP06 5001 Enhanced Black General Purpose Polypropylene PP06 Series polypropylene offer the designer and processor a high performance polymer with well-defined properties in a range of options to suit many applications.The Axpoly® PP06 range of resin co.. |
|||
Particle Size | 3000 µm | 3000 µm | Typical |
Axion Polymers Axpoly® PS02 1000 General Purpose Polystyrene PS02 Series polystyrenes offer the designer and processor a high performance polymer with well-defined properties in a range of options to suit many applications.The Axpoly® PS02 range of resin com.. |
|||
Particle Size | 3000 µm | 3000 µm | Typical |
Axion Polymers Axpoly® PS02 1010 Medium Impact Polystyrene PS02 Series polystyrenes offers the designer and processor a high performance polymer with well-defined properties in a range of options to suit many applications.The Axpoly® PS02 range of resin co.. |
|||
Particle Size | 3000 µm | 3000 µm | Typical |
Axion Polymers Axpoly® PS13 Impact Modified Polystyrene 100% post-consumer recycled polymer (recovered from coat hangers)93% less CO2 impact compared with virgin*Successfully replaces virgin grade resinISO9000 quality certifiedAvailable in black/greyCost.. |
|||
Particle Size | <= 3000 µm | <= 3000 µm | |
BASF Neopolen® P 9270 0.08 g/cc Core density; Expanded Polypropylene (Europe) Description: Neopolen® P 9270 is expanded Polypropylene supplied in the form of beads. The cells are largely closed.Physical properties of moldings made from Neopolen® P 9270.Note: In order to mea.. |
|||
Particle Size | <= 3000 µm | <= 3000 µm | |
BASF Neopolen® P 9270 0.1 g/cc Core density; Expanded Polypropylene (Europe) Description: Neopolen® P 9270 is expanded Polypropylene supplied in the form of beads. The cells are largely closed.Physical properties of moldings made from Neopolen® P 9270.Note: In order to mea.. |
|||
Particle Size | <= 3000 µm | <= 3000 µm | |
BASF Neopolen® P 9280 0.07 g/cc Core density; Expanded Polypropylene (Europe) Description: Neopolen® P 9280 is expanded Polypropylene supplied in the form of beads. The cells are largely closed.Physical properties of moldings made from Neopolen® P 9280.Note: In order to mea.. |
|||
Particle Size | <= 3000 µm | <= 3000 µm | |
BASF Neopolen® P 9280 0.08 g/cc Core density; Expanded Polypropylene (Europe) Description: Neopolen® P 9280 is expanded Polypropylene supplied in the form of beads. The cells are largely closed.Physical properties of moldings made from Neopolen® P 9280.Note: In order to mea.. |
|||
Particle Size | <= 3000 µm | <= 3000 µm | Grain Size |
Gouda Vuurvast CURON 180 T Sp Dense Refractory Castable Description: Curon 180 T special is a tabular alumina based castable, highly resistant against abrasion, dust erosion or heavy impact even at extremely high temperatures.Remarks: These values apply .. |
|||
Particle Size | <= 3000 µm | <= 3000 µm | Grain Size |
Gouda Vuurvast GOLITE 160 GM Refractory Insulating Castable Description: Golite 180 GM is a gunning mix that can be used up to very high temperatures in reducing conditions.Remarks: These values apply to cast products.Information provided by Gouda Vuurvast. |
|||
Particle Size | <= 3000 µm | <= 3000 µm | |
BASF Neopolen® P 9270 0.07 g/cc Core density; Expanded Polypropylene (Europe) Description: Neopolen® P 9270 is expanded Polypropylene supplied in the form of beads. The cells are largely closed.Physical properties of moldings made from Neopolen® P 9270.Note: In order to mea.. |
|||
Particle Size | <= 3000 µm | <= 3000 µm | |
BASF Neopolen® P 9270 0.11 g/cc Core density; Expanded Polypropylene (Europe) Description: Neopolen® P 9270 is expanded Polypropylene supplied in the form of beads. The cells are largely closed.Physical properties of moldings made from Neopolen® P 9270.Note: In order to mea.. |
|||
Particle Size | <= 3000 µm | <= 3000 µm | Grain Size |
Gouda Vuurvast GOLITE 135 GM Refractory Insulating Castable Description: This gunning material can be used in direct contact with open fire and has a high strength.Remarks: These values were obtained from cast samples. These values apply to cast products.Inf.. |