Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Gravity | 1.42 - 1.48 g/cc | 1.42 - 1.48 g/cc | NBR NM-IEC 60811-1-3 |
Karina 02/5-FE-LMP (SDB) Yellow Color Concentrate for PVC Heavy metal free color concentrate recommended for application in electrical wire and cable PVC compounds. Also suitable for pigmentation of flexible and rigid PVC compounds for general purposes. .. |
|||
Specific Gravity | 1.43 - 1.48 g/cc | 1.43 - 1.48 g/cc | ASTM D 792 |
Karina 18/387-RG-GE (CS) Gray Color Concentrate for PVC Heavy metal free color concentrate recommended for application in electrical wire and cable PVC compounds. Also suitable for pigmentation of flexible and rigid PVC compounds for general purposes. .. |
|||
Specific Gravity | 1.42 - 1.48 g/cc | 1.42 - 1.48 g/cc | ASTM D 792 |
Karina 18/90-RG-GE (CS) Gray Color Concentrate for PVC Heavy metal free color concentrate recommended for application in electrical wire and cable PVC compounds. Also suitable for pigmentation of flexible and rigid PVC compounds for general purposes. .. |
|||
Specific Gravity | 1.42 - 1.48 g/cc | 1.42 - 1.48 g/cc | ASTM D 792 |
Karina 18/91-RG-GE (CS) Gray Color Concentrate Heavy metal free color concentrate recommended for application in electrical wire and cable PVC compounds. Also suitable for pigmentation of flexible and rigid PVC compounds for general purposes. .. |
|||
Specific Gravity | 1.42 - 1.48 g/cc | 1.42 - 1.48 g/cc | ASTM D 792 |
Karina 804-02/39-Y-RTC Blue PVC Compound Flame retardant PVC compound recommended for electrical conduit extrusion.Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Specific Gravity | 1.42 - 1.48 g/cc | 1.42 - 1.48 g/cc | ASTM D 792 |
Karina 811-10/23-A-ERYB-PO White PVC Compound PVC powder compound, recommended for extrusion in twin screw extruder of sewer pipes.Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Specific Gravity | 1.42 - 1.48 g/cc | 1.42 - 1.48 g/cc | ASTM D 792 |
Karina 834-48/1-A-ERM-LMP Black PVC Compound Heavy metal free PVC compound recommended for extrusion of automotive profiles.Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Specific Gravity | 1.42 - 1.48 g/cc | 1.42 - 1.48 g/cc | ASTM D 792 |
Karina E 830-10/145-A-ERYB-LMP White PVC Compound Heavy metal free PVC compound recommended for extrusion of profiles for general applications. It is supplied in pellet form and should be processed at the temperature range of 170°C to 190°C... |
|||
Specific Gravity | 1.42 - 1.48 g/cc | 1.42 - 1.48 g/cc | ASTM D 792 |
Karina E 836-10/176-CR White PVC Compound Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Specific Gravity | 1.42 - 1.48 g/cc | 1.42 - 1.48 g/cc | ASTM D 792 |
Karina E 836-10/176-CRA White PVC Compound Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Specific Gravity | 1.42 - 1.48 g/cc | 1.42 - 1.48 g/cc | ASTM D 792 |
Karina E 836-10/185-ERYB White PVC Compound Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Specific Gravity | 1.42 - 1.48 g/cc | 1.42 - 1.48 g/cc | ASTM D 792 |
Karina E 854-10/150-ERYB White PVC Compound Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Specific Gravity | 1.42 - 1.48 g/cc | 1.42 - 1.48 g/cc | ASTM D 792 |
Karina E 854-10/185-ERYB White PVC Compound Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Specific Gravity | 1.42 - 1.48 g/cc | 1.42 - 1.48 g/cc | ASTM D 792 |
Karina E 854-35/1-Y-ERYB Ivory PVC Compound Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Specific Gravity | 1.42 - 1.48 g/cc | 1.42 - 1.48 g/cc | NBR 14288 |
Karina E 855-10/150-ERYB-PO White PVC Compound Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Specific Gravity | 1.42 - 1.48 g/cc | 1.42 - 1.48 g/cc | ASTM D 792 |
Karina 40/296-FC-LMP (CS) Green Color Concentrate for PVC Heavy metal free color concentrate recommended for application in electrical wire and cable PVC compounds. Also suitable for pigmentation of flexible and rigid PVC compounds for general purposes. .. |
|||
Specific Gravity | 1.42 - 1.48 g/cc | 1.42 - 1.48 g/cc | ASTM D 792 |
Karina E 844-10/176-CRB White PVC Compound Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Specific Gravity | 1.44 - 1.48 g/cc | 1.44 - 1.48 g/cc | ASTM D792 |
Compuestos Dominicanos Polycom VY-050775 PVC Compound The Polycom VY series are compounds for the extrusion of both stripes for chaise lounge and flexible window sidings with outstanding weather and outdoes resistance. Also, in the VY series the are p.. |
|||
Specific Gravity | 1.44 - 1.48 g/cc | 1.44 - 1.48 g/cc | ASTM D-792 |
Axiall 124C Moldings & Extrusions Flexible PVC 60C injection molding, plug stock compound. UL approved for 94HB in all colors at a minimum thickness of 3.00 mm.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |
|||
Specific Gravity | 1.44 - 1.48 g/cc | 1.44 - 1.48 g/cc | ASTM D-792 |
Axiall 83-126J Moldings & Extrusions Flexible PVC Flame retardant, 60°C rated injection molding compound.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |
|||
Specific Gravity | 1.44 - 1.48 g/cc | 1.44 - 1.48 g/cc | ASTM D-792 |
Axiall 19890 Wire & Cable Flexible PVC Highly recommended for 105°C, 15 mil wall insulations and jackets where good gasoline and oil resistance is desired.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 201.. |
|||
Specific Gravity | 1.44 - 1.48 g/cc | 1.44 - 1.48 g/cc | ASTM D-792 |
Axiall 83-126K Moldings & Extrusions Flexible PVC Flame retardant, 60°C rated injection molding compound.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |
|||
Specific Gravity | 1.42 - 1.48 g/cc | 1.42 - 1.48 g/cc | ASTM D 792 |
Karina E 840-10/176-CRA White PVC Compound Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Specific Gravity | 1.42 - 1.48 g/cc | 1.42 - 1.48 g/cc | ASTM D 792 |
Karina E 841-08/184-Y-ERYB Beige PVC Compound Information provided by Karina Indústria e Comércio de Plásticos Ltda. |