Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Ashley Polymers Ashlene® R6041 Nylon 66, PTFE and Silicone Modified

Category Polymer , Thermoplastic , Nylon , Nylon 66 , Nylon 66, PTFE Filled
Manufacturer Ashley Polymers
Trade Name Ashlene®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Ashley Polymers Ashlene® R6041 Nylon 66, PTFE and Silicone Modified.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Nylon 66 PTFE and Silicone modified for excellent wear characteristics and low friction.Data provided by the manufacturer
Physical Properties Metric English Comments
Density 1.25 g/cc
0.0452 lb/in³
ASTM D792
Water Absorption 0.80 %
0.80 %
ASTM D570
Linear Mold Shrinkage 0.016 cm/cm
0.016 in/in
ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength, Yield 66.0 MPa
9570 psi
ASTM D638
Elongation at Break 9.0 %
9.0 %
ASTM D638
Flexural Modulus 2.20 GPa
319 ksi
ASTM D790
Izod Impact, Notched 0.370 J/cm
0.693 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Melting Point 260 °C
500 °F
ASTM D3418
Deflection Temperature at 1.8 MPa (264 psi) 102 °C
216 °F
ASTM D648
Users viewing this material also viewed the following: