Ashley Polymers Ashlene® 925LMS-22G Nylon 12, 22% Glass Reinforced

Category Polymer , Thermoplastic , Nylon , Nylon 12 , Nylon 12, 20% Glass Fiber Filled
Manufacturer Ashley Polymers
Trade Name Ashlene®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Ashley Polymers Ashlene® 925LMS-22G Nylon 12, 22% Glass Reinforced.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
A 22% glass reinforced, Molybdenum disulfide filled, Nylon 12 resin for injection molding.Data provided by the manufacturer
Physical Properties Metric English Comments
Density 1.22 g/cc
0.0441 lb/in³
ASTM D792
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 97.0 MPa
14100 psi
ATSM D638
Elongation at Break 3.0 %
3.0 %
ASTM D638
Flexural Modulus 4.00 GPa
580 ksi
ASTM D790
Izod Impact, Notched 1.23 J/cm
2.30 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Melting Point 185 °C
365 °F
ASTM D3418