Thermal Properties | Metric | English | Comments |
---|---|---|---|
Melting Point | 185 - 195 °C | 365 - 383 °F | High melting point |
Oceanchem Group 1,2,5,6,9,10-Hexabromocyclododecane (HBCD) Molecular Formula: C12H18Br6Cas No.: 3194-55-6Characteristics: The product is white crystalline powder, melting point greater than 180°C, bromine content greater than or equal to 73%. This product.. |
|||
Melting Point | 185 °C | 365 °F | |
Radici Heraflex® E 4718 TPC-ET Thermoplastic Elastomer TPC-ET Thermoplastic Elastomer. Low Modulus, Nominal Shore D/15s 43. Natural colorProcessing technology: Injection moldingInformation provided by Radici group. |
|||
Melting Point | 185 °C | 365 °F | Average value: 185 °C Grade Count:8 |
Overview of materials for Nylon 11, Powder This property data is a summary of similar materials in the MatWeb database for the category "Nylon 11, Powder". Each property range of values reported is minimum and maximum values of appropriate M.. |
|||
Melting Point | 185 - 200 °C | 365 - 392 °F | Huntsman/TMA |
Huntsman IROGRAN® A 98 P 4535 TPU-Polyether Excellent resistance to hydrolysis and microbial attack. Suggested for injection molding and extrusion.Information provided by Huntsman |
|||
Melting Point | 185 °C | 365 °F | Peak |
LG Chemical KEYFLEX BT 1033D Ester Type TPE Description: Injection Molding, TPC-ET, General Purpose, Low ModulusApplication: Automotive Interior, Soft Touch GripsCAS: 37282-12-5Information provided by LG Chemical |
|||
Melting Point | 185 - 250 °C | 365 - 482 °F | |
Indium Corp. Indalloy® 138 Pb-Sn-Sb Solder Alloy Information provided by the manufacturer, Indium Corporation. |
|||
Melting Point | 185 °C | 365 °F | DIN 53736 |
Isoflon PA 12 Polyamide 12 General use for mechanical partsGood heat resistanceEasy to useInformation provided by Isoflon. |
|||
Melting Point | 185 - 250 °C | 365 - 482 °F | |
Johnson Matthey JM3070 Soft Solder/Flux General information on the Johnson Matthey soft solder and flux product line: A wide range of Tin/Lead solders suitable for a variety of applications is available from Johnson Matthey. Most materi.. |
|||
Melting Point | 185 - 243 °C | 365 - 469 °F | |
Indium Corp. Indalloy 134 Tin-Lead Solder Alloy Information Provided by Indium Corporation |
|||
Melting Point | 185 °C | 365 °F | ISO 11357-3 |
Suzhou Hipro Polymers Hiprolon® 11 PFB Colorized Nylon powder Hiprolon® 11 PFB colorized is a fluid-bed polyamide powder partly comprised of bio-renewable raw materials. It has excellent weather ability, chemical resistance, wear resistance, impact resistan.. |
|||
Melting Point | 185 °C | 365 °F | 10°C/min; ISO 11357-1/-3 |
DSM Arnitel® EM460 46 Shore D, Injection Molding or Extrusion Grade Copolyester Elastomer (North America) Product description: Arnitel® combines the advantages of engineering thermoplastics, being easy to process with excellent mechanical properties, at the same time with the flexibility of rubbers.Arn.. |
|||
Melting Point | 185 °C | 365 °F | 10°C/min; ISO 11357-1/-3 |
DSM Arnitel® VT3108 TPC-ET Extrusion Grade, High Breathable, Drying of Material Required |
|||
Melting Point | 185 - 195 °C | 365 - 383 °F | DSC |
EMS-Griltech Griltex® D 1655E Copolyester Hotmelt Adhesive (Technical Applications) Description: GRILTEX adhesive products, either in pellet or powdered form, are used to coat apparel interlining substrates. Interlining substrates, coated with GRILTEX adhesive products, provides fo.. |
|||
Melting Point | <= 185 °C | <= 365 °F | Peak Melting Point; ExxonMobil method |
ExxonMobil Escorene™ LD 727.22 Ethylene Vinyl Acetate Copolymer Product Description: Escorene Ultra LD 727.22 is a high vinyl acetate copolymer with a low melting temperature and excellent strength properties and toughness.Availability: North America Additive: .. |
|||
Melting Point | 185 °C | 365 °F | 10°C/min |
Arkema Group Rilsan® Powder D40 Natural Nylon 11, Coating Grade Powder D40 NATURAL - RILSAN POLYAMIDE 11 (PA11) POWDERUnpigmented and clear Powder as an additive for paints. Improves the scratch and abrasion resistance of paints. Allows for different texture d.. |
|||
Melting Point | 185 °C | 365 °F | 10°C/min |
Arkema Group Rilsan® Powder ESY Black X 7260 Nylon 11, Coating Grade Powder ESY BLACK X 7260 - RILSAN POLYAMIDE 11 (PA11) POWDERMelt mix black powder for coating of metallic parts by electrostatic spray, and post fused in an oven.There is a wide range of colors.The p.. |
|||
Melting Point | 185 °C | 365 °F | 10°C/min |
Arkema Group Rilsan® Powder T Blue X 7421 AC Nylon 11, Coating Grade Powder T BLUE X 7421 AC - RILSAN POLYAMIDE 11 (PA11) POWDERBlue Powder pigmented by Dry Blend, designed for the coating of tubes, pipe systems, flanges and fittings for the transport of fluids in pa.. |
|||
Melting Point | 185 °C | 365 °F | 10°C/min |
Arkema Group Rilsan® Powder T GREY 5161 MAC Nylon 11, Coating Grade Powder T GREY 5161 MAC - RILSAN POLYAMIDE 11 (PA11) POWDERMelt mix Grey Powder, designed for the coating of tubes, pipe systems, flanges and fittings for the transport of fluids in particular potabl.. |
|||
Melting Point | 185 °C | 365 °F | 10°C/min |
Arkema Group Rilsan® Powder T NAT BHV COS Nylon 11, Cosmetic Grade Powder T NAT BHV COS - RILSAN POLYAMIDE 11 (PA11) POWDERUnpigmented and clear Powder for the cosmetic industry, used as mild abrasive in 'scrubbing' creams.The properties listed in the dat.. |
|||
Melting Point | 185 °C | 365 °F | 10°C/min |
Arkema Group Rilsan® Powder T NAT BHV RX Nylon 11, Coating Grade Powder T NAT BHV RX - RILSAN POLYAMIDE 11 (PA11) POWDERUnpigmented and clear Powder for the coating of printing rollers.Technical assistance available for any coating process problem.The range inclu.. |
|||
Melting Point | 185 °C | 365 °F | |
BASF Ultramid® 1C PA6/66 (Conditioned) Description: Ultramid® 1C forms flexible, scratch-resistant coatings or tough, resilient, abrasion-resistant coverings on plastics, films, nonwovens, fabrics, leather, paper, wood, or metal.Informa.. |
|||
Melting Point | 185 °C | 365 °F | |
BASF Ultramid® 1C PA6/66 (Dry) Description: Ultramid® 1C forms flexible, scratch-resistant coatings or tough, resilient, abrasion-resistant coverings on plastics, films, nonwovens, fabrics, leather, paper, wood, or metal.Informa.. |
|||
Melting Point | 185 °C | 365 °F | 10°C/min |
Arkema Group Rilsan® Powder T White 7050 Nylon 11, Coating Grade Powder T WHITE 7050 - RILSAN POLYAMIDE 11 (PA11) POWDERWhite powder specially developed for coating of dishwasher baskets. Approved for food contact.Can be applied by dipping the pre heated basket i.. |
|||
Melting Point | 185 °C | 365 °F | ASTM D3418 |
Ashley Polymers Ashlene® 925LS-23G Nylon 12, 23% Glass Reinforced A 23% glass reinforced Nylon 12 resin, with heat stabilizer, for injection molding.Data provided by the manufacturer |
|||
Melting Point | 185 °C | 365 °F | ASTM D789 |
Chem Polymer Formax 605 G Acetal, 5% Glass Reinforced A lubricated, 5% glass reinforced acetal offering a balance of rigidity, dimensional stability and tensile strength.Data provided by the manufacturer, Chem Polymer. |
|||
Melting Point | 185 °C | 365 °F | ASTM D789 |
Chem Polymer Formax 630 G Acetal, 30% Glass Fiber Reinforced A copolymer acetal reinforced with 30% glass fiber for use in applications requiring great strength and rigidity.Data provided by the manufacturer, Chem Polymer. |
|||
Melting Point | 185 °C | 365 °F | ASTM D4591 |
3M Dyneon™ THV 610GZ Fluoroplastic Granules 3M™ Dyneon™ Fluoroplastic Granules THV 610GZ provides a balance of low permeation, thermal stability, and melt processability. It can be used to prepare molded parts and extruded films, tubes, pro.. |
|||
Melting Point | 185 - 195 °C | 365 - 383 °F | Temperature range at which MFI = 10 g/10 min at 21.6 kg.; MQSA 111 |
Lubrizol Advanced Materials Pearlthane® ECO D20N88 Thermoplastic Polyurethane
(discontinued **) PEARLTHANE® ECO D20N88 is a 86 Shore A, High Performance natural TPU based on Renewable Sources with ca. 60% renewable content according to ASTM D6866 for Extrusion and Injection Molding applicatio.. |
|||
Melting Point | 185 °C | 365 °F | DIN 53736 |
Isoflon PA 11 Polyamide 11 General use for mechanical partsGood heat resistanceEasy to useInformation provided by Isoflon. |