Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Ascend Performance Materials Vydyne® 22WSP Nylon 66, Weather Resistant, Conditioned

Category Polymer , Thermoplastic , Nylon , Nylon 66
Manufacturer Ascend Performance Materials (formerly Solutia)
Trade Name VYDYNE®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Ascend Performance Materials Vydyne® 22WSP Nylon 66, Weather Resistant, Conditioned.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Vydyne® 25WSP is a black, weather resistant injection molding grade Nylon 66 resin. These resins offer a well-balanced combination of engineering properties characterized by high strength, rigidity, good toughness, high melt point, good surface lubricity and abrasion resistance. Vydyne 25WSP maintains the chemical resistance typical of nylon to many chemicals, solvents, gasoline, and machine and motor oils.Information provided by Ascend
Physical Properties Metric English Comments
Specific Gravity 1.14 g/cc
1.14 g/cc
ISO 1183
Water Absorption 1.2 %
1.2 %
24 hrs; ISO 62
Moisture Absorption at Equilibrium 2.4 %
2.4 %
Equilibrium at 50%rh; ISO 62
Linear Mold Shrinkage 0.014 cm/cm

@Thickness 2.00 mm
0.014 in/in

@Thickness 0.0787 in
ISO 294-4
Linear Mold Shrinkage, Transverse 0.016 cm/cm

@Thickness 2.00 mm
0.016 in/in

@Thickness 0.0787 in
ISO 294-4
Mechanical Properties Metric English Comments
Tensile Strength, Yield 77.0 MPa
11200 psi
ISO 527
Elongation at Break 60 %
60 %
ISO 527
Elongation at Yield 25 %
25 %
ISO 527
Tensile Modulus 1.55 GPa
225 ksi
ISO 527
Flexural Strength 22.0 MPa
3190 psi
ISO 178
Flexural Modulus 1.40 GPa
203 ksi
ISO 178
Thermal Properties Metric English Comments
Melting Point 260 °C
500 °F
ISO 3146