Techmer ES HiFill® PA6 IM 0240 Impact Modified

Category Polymer , Thermoplastic , Nylon , Nylon 6 , Nylon 6, Impact Grade
Manufacturer Techmer ES
Trade Name HiFill®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Techmer ES HiFill® PA6 IM 0240 Impact Modified.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Availability: North AmericaForms: PelletsFiller/Reinforcement: Unspecified Filler/ReinforAdditive: Impact ModifierFeatures: High Density and Impact ModifiedProcessing Method: Injection MoldingInformation provided by TP Composites, Inc.
Physical Properties Metric English Comments
Density 2.40 g/cc
0.0867 lb/in³
ASTM D792
Water Absorption 0.40 %

@Time 86400 sec
0.40 %

@Time 24.0 hour
ASTM D570
Linear Mold Shrinkage, Flow 0.0050 cm/cm

@Thickness 3.17 mm
0.0050 in/in

@Thickness 0.125 in
ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength 59.3 MPa
8600 psi
ASTM D638
Elongation at Yield 4.0 %
4.0 %
ASTM D638
Flexural Yield Strength 96.5 MPa
14000 psi
ASTM D790
Flexural Modulus 6.55 GPa
950 ksi
ASTM D790
Izod Impact, Notched 1.23 J/cm

@Thickness 3.17 mm
2.30 ft-lb/in

@Thickness 0.125 in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 152 °C
305 °F
Unannealed; ASTM D648