Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 1.55 GPa | 225 ksi | STN EN ISO 527-2 |
Plastcom PLASTALEN® PC 69 T 10 003/1M Polypropylene reinforced with mineral filler Modified PP copolymer for injection molding with the content of 10% mineral filler. Application in all automotive industry. Delivered in black.Information Provided by Plastcom spol. s r.o. |
|||
Tensile Modulus | 1.55 GPa | 225 ksi | Type I, 5.1 mm/min; ASTM D638 |
PolyOne LubriOne™ PC-20GF/15T Polycarbonate (PC) LubriOne™ Lubricated and Wear-Resistant Compounds have been specifically formulated to be self-lubricating materials, offering low coefficient of friction and improved wear resistance properties. L.. |
|||
Tensile Modulus | 1.55 GPa | 225 ksi | ISO 527-1/-2 |
Quadrant EPP Borotron® HM PE-HMW + boron based additive (ISO Data) Borotron UH and Borotron HM are boron loaded PE-(U)HMW grades, specifically developed for neutron shielding purposes in nuclear installations. The high hydrogen content of PE-(U)HMW makes it very su.. |
|||
Tensile Modulus | 1.55 GPa | 225 ksi | |
Radici Radilon® A ECP3808 (cond.) Nylon 66 Radilon® A is a range of polyamide 66 (PA66) products obtained through the polymerization of hexamethylendiamine and adipic acid, and used for injection, extrusion and blow-molding.Information prov.. |
|||
Tensile Modulus | 1.55 GPa | 225 ksi | ASTM D638 |
Fiberfil® J-60/GB/20 Polypropylene Homopolymer, 20% Glass beads Information provided by FIBERFIL Engineered Plastics |
|||
Tensile Modulus | 1.55 GPa | 225 ksi | ASTM D638 |
Fiberfil® PP-60/V2 Polypropylene Homopolymer, Flame Retardant, UL94 V2 Information provided by FIBERFIL Engineered Plastics |
|||
Tensile Modulus | 1.55 GPa | 225 ksi | DIN 53457 |
Isoflon PA 12 Polyamide 12 General use for mechanical partsGood heat resistanceEasy to useInformation provided by Isoflon. |
|||
Tensile Modulus | 1.55 GPa | 225 ksi | ISO 527 |
Styrolution PS ESCRimo HIPS Styrolution PS ESCRimo is a high impact polystyrene grade with an improved stress cracking resistance compared to conventional high impact polystyreneHigh ESCR resistanceDeep draw thermoformingUL 94.. |
|||
Tensile Modulus | 1.55 GPa | 225 ksi | 1mm/min; ISO 527-2 |
Borealis BG373MO Polypropylene Copolymer BG373MO is a heterophasic copolymer. Products molded with this grade exhibit excellent antistatic performance and very good mould release. Electrostatic charge is |
|||
Tensile Modulus | 1.55 GPa | 225 ksi | At 1 mm/min; ISO 527-2 |
Borealis Daplen™ HJ060UB Polypropylene Compound for Direct Left Manufactured Applications Daplen FJ060UB is a special low viscosity compound for direct LFT manufacturing process. It interacts perfectly with glass fibers to create excellent stiffness and impact resistance. Daplen HJ060U.. |
|||
Tensile Modulus | 1.55 GPa | 225 ksi | ISO 527 |
Borealis Daploy™ WF420HMS High Melt Strength Polypropylene for Extrusion Coating Daploy WF420HMS resin is a propylene-based, structurally isomeric polymer, which combines significantly increased melt strength with largely drawability of the polymer melt. Thus, the material is g.. |
|||
Tensile Modulus | 1.55 GPa | 225 ksi | ISO 527-2 |
Total PPH 3060 Polypropylene, Homopolymer ATOFINA Polypropylene PPH 3060 is homopolymer.ApplicationATOFINA Polypropylene PPH 3060 is characterized by a low fluidity for continuous extrusion of strapping, rope fibers and high tenacity tapes .. |
|||
Tensile Modulus | 1.55 GPa | 225 ksi | ISO 527-2 |
Total PPH 7060 Polypropylene, Homopolymer ATOFINA Polypropylene PPH 7060 is homopolymer.ApplicationATOFINA Polypropylene PPH 7060 is intended for the injection molding of packaging containers, toys, domestic appliances, garden furniture and.. |
|||
Tensile Modulus | 1.55 GPa | 225 ksi | ISO 527-2 |
Total PPH 7062 Polypropylene, Homopolymer ATOFINA Polypropylene PPH 7062 is an antistatic homopolymer.ApplicationATOFINA Polypropylene PPH 7062 is intended for injection molding applications of boxes, closures and household articles. Inform.. |
|||
Tensile Modulus | 1.55 GPa | 225 ksi | ISO 527-2 |
Total PPH 7069 Polypropylene, Homopolymer ATOFINA Polypropylene PPH 7069 is homopolymer.ApplicationATOFINA Polypropylene PPH 7069 is characterized by medium fluidity for extrusion of continuous filament (CF) and bulk continuous filament (BC.. |
|||
Tensile Modulus | 1.55 GPa | 225 ksi | ISO 527-2 |
Total PPH 8069 Polypropylene, Homopolymer ATOFINA Polypropylene PPH 8069 is homopolymer.ApplicationATOFINA Polypropylene PPH 8069 has been developed for the production of staple fibers for non-wovens. PPH 8069 has a special anti gas-fading.. |
|||
Tensile Modulus | 1.55 GPa | 225 ksi | ASTM D638 |
Eastman Tritan MX710 Copolyester Eastman Tritan Copolyester MX710 is an amorphous product with excellent appearance and clarity. Eastman Tritan Copolyester MX710 has many outstanding features that include excellent toughness, hydr.. |
|||
Tensile Modulus | 1.55 GPa | 225 ksi | ASTM D638 |
Eastman Tritan TX1000 Copolyester Eastman Tritan TX1000 is an amorphous copolyester with excellent appearance and clarity. Its most outstanding features are excellent toughness, hydrolytic stability, and heat and chemical resistanc.. |
|||
Tensile Modulus | 1.55 GPa | 225 ksi | ASTM D638 |
Eastman Tritan TX1001 Copolyester Eastman Tritan TX1001 is an amorphous copolyester with excellent appearance and clarity. Eastman Tritan TX1001 contains a mold release derived from vegetable based sources. Its most outstanding fe.. |
|||
Tensile Modulus | 1.55 GPa | 225 ksi | ASTM D638 |
CPC - Vycom FLAMETEC™ KYTEC® PVDF Kytec® PVDF, the homopolymer of 1, 1-difluoroethene, is a tough engineering thermoplastic that offers a unique balance of properties. Kytec has the characteristic stability of fluoropolymers when e.. |
|||
Tensile Modulus | 1.55 GPa | 225 ksi | ISO 527-2 |
Domo 1100N Polypropylene Homopolymer Information provided by Domo. |
|||
Tensile Modulus | 1.55 GPa | 225 ksi | ISO 527-2 |
Domo 1101N Polypropylene Homopolymer Information provided by Domo. |
|||
Tensile Modulus | 1.55 GPa | 225 ksi | |
BASF Novolen® 1100 UC Polypropylene, Injection Molding Grade Injection molded partsData was collected by ISO methods and provided by BASF. |
|||
Tensile Modulus | 1.55 GPa | 225 ksi | 1 mm/min |
Arkema Group Orgalloy® LE 60HM Flexible Nylon Alloy (Conditioned) LE series, flexible polyamide alloys: processability on PE screw, low moisture absorption, chemical resistance (no known solvents).higher in rigidity than LE 6000. For film, hollow vessel blow moldi.. |
|||
Tensile Modulus | 1.55 GPa | 225 ksi | ISO 527-2 |
Ascend Performance Materials Vydyne® 25WSP Nylon 66, Conditioned (2.5% Moisture) Vydyne® 25WSP is a black, weather resistant injection molding grade Nylon 66 resin. These resins offer a well-balanced combination of engineering properties characterized by high strength, rigidity.. |
|||
Tensile Modulus | 1.55 GPa | 225 ksi | 1mm/min; ISO 527 |
BASF Ultraform N 2640 Z4 BK140 Q600 POM Ultraform N2640 Z4 BK140 Q600 is a high toughness, elastomer-modified injection molding POM grade. |
|||
Tensile Modulus | 1.55 GPa | 225 ksi | |
BASF Novolen® 1100 N Polypropylene, Injection Molding Grade Grade for injection molded parts. Also available as a special grade for fibers (short spinning) and cast film.Data was collected by ISO methods and provided by BASF. |
|||
Tensile Modulus | 1.55 GPa | 225 ksi | |
BASF Novolen® 1100 VC Polypropylene Data was collected by ISO methods and provided by BASF. |
|||
Tensile Modulus | 1.55 GPa | 225 ksi | roll stack films TD; ISO 527-3 |
Borealis Bormod™ HC904CF Polypropylene Bormod™ BJ368MO is a polypropylene copolymer characterized by good flow, and optimum combination of high stiffness and high impact strength. The material is nucleated with Borstar® Nucleation Tech.. |
|||
Tensile Modulus | 1.55 GPa | 225 ksi | 1 mm/min |
Polimeri Europa SINKRAL C423/M3 ABS
(discontinued **) Symbol according to ISO 1043-1: ABS Grade designation according to ISO 2580-ABS 1,MG,95-08-16-15 Special low gloss grade for injection moulding. Good impact resistance coupled with good flow permi.. |