Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Asahi Kasei Thermofil P6-30FM-0801 30% Fiber Mineral Filled, Heat Stabilized

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene, Mineral Reinforced, Impact Modified
Manufacturer Asahi Kasei
Trade Name Thermofil
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Asahi Kasei Thermofil P6-30FM-0801 30% Fiber Mineral Filled, Heat Stabilized.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by Asahi Thermofil
Physical Properties Metric English Comments
Specific Gravity 1.13 g/cc
1.13 g/cc
ASTM D792
Melt Flow 7.7 g/10 min
7.7 g/10 min
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 65.8 MPa
9550 psi
ASTM D638
Elongation at Yield 4.0 %
4.0 %
ASTM D638
Flexural Strength 97.2 MPa
14100 psi
ASTM D790
Flexural Modulus 4.55 GPa
660 ksi
ASTM D790
Izod Impact, Notched 0.587 J/cm
1.10 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 146 °C
295 °F
ASTM D648
Users viewing this material also viewed the following:
Copyright © lookpolymers.com All Rights Reserved