Arlon 55503R062 0.062" Cured Silicone Rubber with Fiberglass Substrate

Category Polymer , Thermoset , Silicone , Silicone, Molded, Glass Fiber Filled
Manufacturer Arlon
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Arlon 55503R062 0.062" Cured Silicone Rubber with Fiberglass Substrate.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Design/Construction:Interleave: 3 mil PolyethyleneSide 1: Cured Silicone RubberSubstrate: Prime Coated 162 Style FiberglassSide 2: Cured Silicone RubberThis data represents typical values for the production material and should not be used as material specifications.Information provided by ARLON Silicone Technologies Division.
Physical Properties Metric English Comments
Thickness 457 microns
18.0 mil
Substrate
559 microns
22.0 mil
Side 1
559 microns
22.0 mil
Side 2
1570 microns
62.0 mil
Overall Thickness
Mechanical Properties Metric English Comments
Hardness, Shore A 50
50
Silicone Property
Tensile Strength >= 7.58 MPa
>= 1100 psi
Silicone Property
Elongation at Break >= 600 %
>= 600 %
Silicone Property
Thermal Properties Metric English Comments
Maximum Service Temperature, Inert 232 °C
450 °F
Minimum Service Temperature, Air -56.7 °C
-70.0 °F
Electrical Properties Metric English Comments
Dielectric Strength >= 15.7 kV/mm
>= 400 kV/in
Processing Properties Metric English Comments
Shelf Life 12.0 Month
12.0 Month
Descriptive Properties Value Comments
Color Red
Total Product Weight (oz/yd2) 57.5
Uncoated Fabric Break Strength (lb/in) 420
Fill Direction
700
Warp Direction