Material Notes:
Low ModulusProduct Color: RedInterleave: 0.003" PolyethyleneThis data represents typical values for the production material and should not be used as material specifications.Information provided by ARLON Silicone Technologies Division.
Physical Properties Metric English Comments
Thickness 3180 microns
125 mil
Overall
Mechanical Properties Metric English Comments
Hardness, Shore A 35 - 45
35 - 45
Tensile Strength >= 6.89 MPa
>= 1000 psi
Elongation at Break >= 700 %
>= 700 %
100% Modulus 0.00103 GPa
0.150 ksi
Tear Strength >= 35.1 kN/m
>= 200 pli
Compression Set <= 28 %
<= 28 %
After post cure
Thermal Properties Metric English Comments
Maximum Service Temperature, Inert 232 °C
450 °F
Minimum Service Temperature, Air -56.7 °C
-70.0 °F
Electrical Properties Metric English Comments
Dielectric Strength >= 15.7 kV/mm
>= 400 kV/in
Processing Properties Metric English Comments
Shelf Life 12.0 Month

@Temperature 4.44 °C
12.0 Month

@Temperature 40.0 °F
Descriptive Properties Value Comments
Total Product Weight (oz/yd2) 105
Users viewing this material also viewed the following: