Mechanical Properties | Metric | English | Comments |
---|---|---|---|
100% Modulus | 0.00103 GPa | 0.150 ksi | |
TSE Industries Millathane® HT High Temperature-Resistant Millable Polyester Polyurethane with 20 PHR N990 (MT) Filler MILLATHANE HT is a polyester millable polyurethane which has the ability to withstand elevated temperatures. Polyurethanes have been known for their excellent resistance to abrasion, impact, tear st.. |
|||
100% Modulus | >= 0.00103 GPa | >= 0.150 ksi | catalyzed |
ACC QSil 551 QSI Quantum Silicones Silicone Potting Material
(discontinued **) Part of the Amber Chemical Group. Data provided by manufacturer.Characteristics: 100% solid, long pot life, low modulus, good elongation. |
|||
100% Modulus | 0.00103 GPa | 0.150 ksi | |
TSE Industries Millathane® HT High Temperature-Resistant Millable Polyester Polyurethane with 20 PHR N990 (MT) Filler MILLATHANE HT is a polyester millable polyurethane which has the ability to withstand elevated temperatures. Polyurethanes have been known for their excellent resistance to abrasion, impact, tear st.. |
|||
100% Modulus | 0.00103 GPa | 0.150 ksi | ASTM D 412 |
CPT C-Flex® R70-001 Opaque Biocompatible TPE C-Flex® is a family of patented thermoplastic elastomers which range in hardness from 5 shore A to 95 shore A. C-Flex® TPE's are biocompatible polymer blends which meet or exceed the current.. |
|||
100% Modulus | 0.00103 GPa | 0.150 ksi | |
Arlon 10842N125 Cured/Post-cured, Unsupported Silicone Rubber Low ModulusProduct Color: Natural (Transparent)Interleave: 0.003" PolyethyleneThis data represents typical values for the production material and should not be used as material specifications.Inform.. |
|||
100% Modulus | 0.00103 GPa | 0.150 ksi | |
Arlon 10842R125 Cured/Post-cured, Unsupported Silicone Rubber Low ModulusProduct Color: RedInterleave: 0.003" PolyethyleneThis data represents typical values for the production material and should not be used as material specifications.Information provided by .. |
|||
100% Modulus | 0.00103 GPa | 0.150 ksi | |
Arlon 10842S125 Cured/Post-cured, Unsupported Silicone Rubber Low ModulusProduct Color: Saddle BrownInterleave: 0.003" PolyethyleneThis data represents typical values for the production material and should not be used as material specifications.Information pro.. |
|||
100% Modulus | 0.00103 GPa | 0.150 ksi | Silicone Property |
Arlon 30850S125 0.125" Uncured, Unsupported Silicone Rubber on a Kodacel Carrier Design/Construction:Side 1: Uncured, Unsupported Silicone RubberSubstrate: Kodacel CarrierInterleave: 0.003" PolyethyleneThis data represents typical values for the production material and should.. |
|||
100% Modulus | 0.00103 GPa | 0.150 ksi | Silicone Property |
Arlon 30850N125 0.125" Uncured, Unsupported Silicone Rubber on a Kodacel Carrier Design/Construction:Side 1: Uncured, Unsupported Silicone RubberSubstrate: Kodacel CarrierInterleave: 0.003" PolyethyleneThis data represents typical values for the production material and should.. |