Material Notes:
Designation ISO 1874-PA11/xx,F,THL,22-020Transparent semi-crystalline PA11 grade.Used for film extrusion and injection molding (low thickness).Very good low temperature impact strength.High chemical resistance.ISO data provided by the manufacturer, Arkema.
Physical Properties Metric English Comments
Density 1.04 g/cc
0.0376 lb/in³
Mechanical Properties Metric English Comments
Tensile Strength, Yield 54.0 MPa
7830 psi
50 mm/min
Elongation at Break >= 50 %
>= 50 %
Nominal Strain; 50 mm/min
Elongation at Yield 6.0 %
6.0 %
50 mm/min
Tensile Modulus 1.53 GPa
222 ksi
1 mm/min
Charpy Impact Unnotched NB
NB
NB
NB
Low Temp
Charpy Impact, Notched 1.25 J/cm²

@Temperature -30.0 °C
5.95 ft-lb/in²

@Temperature -22.0 °F
Thermal Properties Metric English Comments
Melting Point 183 °C
361 °F
(Dry)
Optical Properties Metric English Comments
Transmission, Visible 80 %
80 %
Mfr. reports 'Transparent' but doesn't quantify.