Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Arkema Group Rilsan® BMV 400 TL Nylon 11 (Dry)

Category Polymer , Thermoplastic , Nylon , Nylon 11 , Nylon 11, Unreinforced
Manufacturer Arkema
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Arkema Group Rilsan® BMV 400 TL Nylon 11 (Dry).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Designation ISO 1874-PA11,M,18-002,ZFlexible grade for injection molding. Available color: natural. Light and heat stabilized. Plasticizing agent free.Outstanding impact strength and tear spreading at low temperature. Good abrasion resistance. Low shrinkage: include 1% on average for the design of the mold. Good dimensional stability (low moisture absorption).Example applications: Mechanical parts with impact and vibrations resistance.ISO data provided by the manufacturer, Arkema.
Physical Properties Metric English Comments
Density 1.00 g/cc
0.0361 lb/in³
Water Absorption 1.3 %
1.3 %
Mechanical Properties Metric English Comments
Tensile Strength, Yield 18.0 MPa

@Strain 50.0 %
2610 psi

@Strain 50.0 %
50 mm/min
Elongation at Break >= 50 %
>= 50 %
Nominal Strain; 50 mm/min
Tensile Modulus 0.195 GPa
28.3 ksi
1 mm/min
Charpy Impact Unnotched NB
NB
NB
NB
Low Temp
Charpy Impact, Notched NB
NB
1.80 J/cm²

@Temperature -30.0 °C
8.57 ft-lb/in²

@Temperature -22.0 °F
Thermal Properties Metric English Comments
Melting Point 175 °C
347 °F
10°C/min
Flammability, UL94 HB

@Thickness 1.60 mm
HB

@Thickness 0.0630 in
HB

@Thickness 3.10 mm
HB

@Thickness 0.122 in
Users viewing this material also viewed the following: