Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Arkema Group Pebax® 5533 SN 70 NOIR Polyether Block Amide (PEBA) (Conditioned)

Category Polymer , Thermoplastic , Elastomer, TPE , Polyether Block Amide (PEBA)
Manufacturer Arkema
Trade Name Pebax®
Port Ningbo port,China
Trade Terms EXW, FOB, CFR, CIF
Payment Terms L/C, T/T, PayPal
Download PDF Arkema Group Pebax® 5533 SN 70 NOIR Polyether Block Amide (PEBA) (Conditioned).pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
POLYETHER BLOCK AMIDE (PEBA) Hardness 60 shore D Black antistatic grade Applications: Tube extrusion...ISO data provided by the manufacturer, Arkema.
Physical Properties Metric English Comments
Density 1.09 g/cc
0.0394 lb/in³
Melt Flow 5.0 g/10 min
<br>@Load 5.00 kg,<br> Temperature 250 °C
5.0 g/10 min
<br>@Load 11.0 lb,<br> Temperature 482 °F
Mechanical Properties Metric English Comments
Hardness, Shore D 60
60
Tensile Strength, Yield 17.0 MPa
2470 psi
50 mm/min
Elongation at Break >= 50 %
>= 50 %
Nominal Strain; 50 mm/min
Elongation at Yield 36 %
36 %
50 mm/min
Tensile Modulus 0.298 GPa
43.2 ksi
1 mm/min
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 220 µm/m-°C
<br>@Temperature 20.0 °C
122 µin/in-°F
<br>@Temperature 68.0 °F
Melting Point 159 °C
318 °F
(Dry)
Vicat Softening Point 144 °C
291 °F
50°C/hr; 50N
Flammability, UL94 HB
<br>@Thickness 1.60 mm
HB
<br>@Thickness 0.0630 in
HB
<br>@Thickness 3.20 mm
HB
<br>@Thickness 0.126 in
Electrical Properties Metric English Comments
Surface Resistance 5500 ohm
5500 ohm