Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Arkema Group Pebax® 3533 SN 01 Polyether Block Amide (PEBA) (Conditioned)

Category Polymer , Thermoplastic , Elastomer, TPE , Polyether Block Amide (PEBA)
Manufacturer Arkema
Trade Name Pebax®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Arkema Group Pebax® 3533 SN 01 Polyether Block Amide (PEBA) (Conditioned).pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
POLYETHER BLOCK AMIDE (PEBA) hardness 35 shore D Non plasticized flexible Polyamide Outstanding mechanical properties at low temperature (-40°C) Applications: molded parts for sport goods (softness, nice touch feeling) Industrial (damping properties, overmolding, resiliency)ISO data provided by the manufacturer, Arkema.
Physical Properties Metric English Comments
Density 1.01 g/cc
0.0365 lb/in³
Melt Flow 12 g/10 min

@Load 1.00 kg,
Temperature 235 °C
12 g/10 min

@Load 2.20 lb,
Temperature 455 °F
Mechanical Properties Metric English Comments
Hardness, Shore D 35
35
Tensile Strength, Yield 3.70 MPa

@Strain 50.0 %
537 psi

@Strain 50.0 %
50 mm/min
Tensile Modulus 0.0150 GPa
2.18 ksi
1 mm/min
Charpy Impact Unnotched NB
NB
NB
NB
Low Temp
Charpy Impact, Notched NB
NB
NB
NB
Low Temp
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 210 µm/m-°C

@Temperature 20.0 °C
117 µin/in-°F

@Temperature 68.0 °F
Melting Point 144 °C
291 °F
(Dry)
Deflection Temperature at 0.46 MPa (66 psi) 46.0 °C
115 °F
Vicat Softening Point 74.0 °C
165 °F
50°C/hr; 50N
Flammability, UL94 HB

@Thickness 1.60 mm
HB

@Thickness 0.0630 in
Optical Properties Metric English Comments
Transmission, Visible 80 %
80 %
Mfr. reports 'Transparent' but doesn't quantify.
Electrical Properties Metric English Comments
Surface Resistance 3.00e+12 ohm
3.00e+12 ohm
Users viewing this material also viewed the following: