Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 32.69 MPa | 4742 psi | 50 mm/min; ASTM D638 |
Amco PRIMATOP PP CO 120-11 RC Random Copolymer Features:medium flowcontains clarifying agentexcellent clarityApplications:storage boxesvialscontainersFormer A-Top Polymers product; part of Amco product line since 2013. |