Adell RR-18 Copolymer Polypropylene, 40% Glass Reinforced

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene with 40% Glass Fiber Filler
Manufacturer Adell Plastics, Inc.
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Adell RR-18 Copolymer Polypropylene, 40% Glass Reinforced.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Data provided by Adell Plastics, Inc.
Physical Properties Metric English Comments
Density 1.22 g/cc
0.0441 lb/in³
ASTM D792
Water Absorption 0.030 %
0.030 %
24 hour immersion; ASTM D570
Linear Mold Shrinkage 0.0035 cm/cm
0.0035 in/in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Rockwell M 58
58
ASTM D785
Hardness, Rockwell R 110
110
ASTM D785
Tensile Strength, Ultimate 82.1 MPa
11900 psi
ASTM D638
Elongation at Break 4.5 %
4.5 %
ASTM D638
Flexural Strength 110 MPa
16000 psi
ASTM D790
Flexural Modulus 5.10 GPa
740 ksi
ASTM D790
Izod Impact, Notched 1.30 J/cm
2.44 ft-lb/in
ASTM D256
Izod Impact, Unnotched 5.90 J/cm
11.1 ft-lb/in
ASTM D256
Gardner Impact 0.700 J
0.516 ft-lb
ASTM D3029
Thermal Properties Metric English Comments
Melting Point 160 °C
320 °F
ASTM D789
Deflection Temperature at 0.46 MPa (66 psi) 157 °C
315 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 149 °C
300 °F
ASTM D648
Flammability, UL94 HB