Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Wellman Wellamid® MR410 22H-NBK1 40% Mineral Reinforced Nylon 66

Category Polymer , Thermoplastic , Nylon , Nylon 66 , Nylon 66, 40% Mineral Filled
Manufacturer Wellman Engineering Resins
Trade Name Wellamid®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Wellman Wellamid® MR410 22H-NBK1 40% Mineral Reinforced Nylon 66.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: Mineral Reinforced Nylon 66Information provided by Wellman.
Physical Properties Metric English Comments
Density 1.49 g/cc
0.0538 lb/in³
ISO 1183-87
Filler Content 40 %
40 %
Linear Mold Shrinkage, Flow 0.0050 - 0.0090 cm/cm
0.0050 - 0.0090 in/in
ISO DIS 294-4
Linear Mold Shrinkage, Transverse 0.010 - 0.014 cm/cm
0.010 - 0.014 in/in
ISO DIS 294-4
Mechanical Properties Metric English Comments
Tensile Strength at Break 75.0 MPa
10900 psi
ISO 527-93
Elongation at Break 3.0 %
3.0 %
ISO 527-93
Flexural Strength 130 MPa
18900 psi
ISO 178-93
Flexural Modulus 6.835 GPa
991.3 ksi
ISO 178-93
Izod Impact, Notched (ISO) 3.32 kJ/m²
1.58 ft-lb/in²
ISO 180-93
Thermal Properties Metric English Comments
Melting Point 260 °C
500 °F
ISO 3146
Deflection Temperature at 1.8 MPa (264 psi) 160 °C
320 °F
ISO 75-93