Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 5.10 GPa | 740 ksi | Tangent; ASTM D790 |
RheTech Products F38-04 35% Glass Fiber/Mineral Co-Reinforced Polypropylene, Chemically Coupled, White Applications: HousingsBracketsSupport ductsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Flexural Modulus | 5.10 GPa | 740 ksi | |
Plastcom SLOVAMID 66 T 15 PA66, 15% mineral filling FeaturesPA 66 with the content of 15 % chemically modified mineral filling. Used for holders of electric hand tools, for hobby tools, gears, covers of electric tools, flat products, automobile wheel.. |
|||
Flexural Modulus | 5.10 GPa | 740 ksi | ISO 178 |
Nilit FRIANYL A63 FK 1020 Nylon 6.6 for injection molding, 10% glass fiber and 20% glass ball reinforced Nylon 6.6 for injection moldingInformation provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Flexural Modulus | 5.10 GPa | 740 ksi | ISO 178 |
Nilit FRIANYL A63 HH-FK 1020 Nylon 6.6 for injection molding, 10% glass fiber and 20% glass ball reinforced Nylon 6.6 for injection moldingInformation provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Flexural Modulus | 5.10 GPa | 740 ksi | ISO 178 |
Nilit FRIANYL B63 L-HS-GV30 Nylon 6 for injection molding, 30% glass fiber reinforced Nylon 6 for injection molding, improved fluidity, high impact modified.Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Flexural Modulus | 5.10 GPa | 740 ksi | ASTM Data |
BASF Capron® SEG3 H1 15% Glass-Filled Nylon 6 (Dry)
(discontinued **) Capron SEG3 H1 is a 15% glass reinforced nylon 6 injection molding compound exhibiting. It exhibits exceptional surface aesthetics at the slower fill speeds associated with the gas assist injection .. |
|||
Flexural Modulus | 5.10 GPa | 740 ksi | |
Plastcom SLOVALEN PH 69 GF 30 LS PP, 30% glass fibre, mod. of mech. prop., UV stability FeaturesModified homopolymer PP for injection moulding, chemically reinforced with 30% glass fibre, contains the modifier of mechanical properties. UV stable. Increased strength in comparison with u.. |
|||
Flexural Modulus | 5.10 GPa @Temperature 90.0 °C |
740 ksi @Temperature 194 °F |
ASTM D790 |
LATI LARIL 13 G/20 20% Glass Fiber Reinforced Polyphenylene Oxide (PPOm)
(Unverified Data**) Description: Laril thermoplastics are polyphenylene oxide (PPOm) products. They exhibit excellent toughness, even at low temperatures, good thermal resistance and dimensional stability are the most .. |
|||
Flexural Modulus | 5.10 GPa | 740 ksi | ISO 178 |
SABIC Innovative Plastics LNP LUBRICOMP DFL23 PC LNP* Lubricomp* DFL23 is a compound based on Polycarbonate resin containing 15% Glass Fiber and 10% PTFE. Added features include: Internally Lubricated. |
|||
Flexural Modulus | 5.10 - 9.31 GPa | 740 - 1350 ksi | Average value: 7.66 GPa Grade Count:17 |
Overview of materials for Polyphenylene Sulfide (PPS) with 20% Glass Fiber Filler This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS) with 20% Glass Fiber Filler". Specific grades with glass content between 15%.. |
|||
Flexural Modulus | 5.10 GPa | 740 ksi | ASTM D790 |
Global GPP-240C 40% Glass Reinforced, Chemically Coupled Impact Polypropylene Information provided by Global Polymers Corporation. |
|||
Flexural Modulus | 5.10 GPa | 740 ksi | 2.6 mm/min, 100 mm span; ASTM D 790 |
SABIC Innovative Plastics Ultem 2212 PEI 20% Milled glass filled, enhanced flow Polyetherimide (Tg 217C). ECO Conforming, UL94 V0 and 5VA listing.This data was supplied by SABIC-IP for the Americas region. |
|||
Flexural Modulus | 5.10 GPa | 740 ksi | 2.6 mm/min, 100 mm span; ASTM D790 |
SABIC Innovative Plastics ULTEM 2212EPR PEI (Asia Pacific) 20% Milled glass filled, high flow Polyetherimide (Tg 217C) with internal mold release and enhanced electroplatability. ECO Conforming, UL94 V0 and 5VA lising. |
|||
Flexural Modulus | 5.10 GPa | 740 ksi | 2.6 mm/min, 100 mm span; ASTM D790 |
SABIC Innovative Plastics ULTEM 2212R PEI 20% Milled glass filled, enhanced flow Polyetherimide (Tg 217C) with internal mold release. ECO Conforming, UL94 V0 and 5VA listing. |
|||
Flexural Modulus | 5.10 GPa | 740 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Valox® EH7025AG PBT+PET Valox EH7025AG is a mineral filled PBT/PET that offers good surface appearance, good flow and good heat performance. EH7025AG was developed for automotiove bezel application. |
|||
Flexural Modulus | 5.10 GPa | 740 ksi | ASTM D790 |
Chase Plastics CP Pryme® N140MGHSL (COND, 50% RH) Nylon 6, 40% Mineral/Glass Reinforced, Heat Stabilized, Internally Lubricated Information provided by Chase Plastics. |
|||
Flexural Modulus | 5.10 GPa | 740 ksi | ISO 178-93 |
Wellman Wellamid® GF13-66 XE-NBK1 13% Glass Fiber Reinforced, Engineering Grade Nylon 66 Description: Glass Fiber Reinforced, Engineering Grade Nylon 66Information provided by Wellman. |
|||
Flexural Modulus | 5.10 GPa | 740 ksi | ISO 178 |
Wellman Wellamid® GF14-60 XE-N 14% Glass Fiber Reinforced Nylon 6, Lubricated & Heat Stabilized Typical Applications: Radio and TV components, dishwasher roller carriages, chain saw oil reservoirs, gears, housings, door & window latches, power hand tool housings, high temperature devices.Data .. |
|||
Flexural Modulus | 5.10 GPa | 740 ksi | ISO 178-93 |
Wellman Wellamid® GFT1628-BK 17% Glass Fiber Reinforced, Impact Modified Nylon 66 Description: Glass Fiber Reinforced, Impact Modified Nylon 66Information provided by Wellman. |
|||
Flexural Modulus | 5.10 GPa | 740 ksi | DIN 52457 |
CP-Polymer-Technik Wellamid® 6000 GVS 10/20 HWCP 10% Glass Fiber and 20% Glass Sphere Nylon 6, Heat Stabilized, Dry Information provided by CP-Polymer-Technik GmbH & Co. KG |
|||
Flexural Modulus | 5.10 GPa | 740 ksi | ISO 178 |
Eurostar Starflam PK0052E PA6, 25% Mineral Filled, Injection Molded PK0052E is a Halogen Free and Red Phosphorous Free, Flame Retardant, Mineral Filed, Polyamide 6 Injection Molding (also known as PM3520Z222 or PA 25E6 U9 Z22)Information provided by Polymer Technolo.. |
|||
Flexural Modulus | 5.10 GPa | 740 ksi | ISO 178 |
CENTROPLAST CENTROTRON GF 15 Polyphenylene sulfide 15% glass fiber CENTROTRON is a plastic that is resistant to oxidation and hydrolysis which can be used in high temperature applications. CENTROTRON has a low sliding friction coefficient and high abrasion resista.. |
|||
Flexural Modulus | 5.10 GPa | 740 ksi | ASTM D790 |
Asahi Kasei Thermylene® P6-30FG-0632 30% Glass Fiber Reinforced, Heat Stabilized Information provided by Asahi Thermofil |
|||
Flexural Modulus | 5.10 GPa | 740 ksi | ISO Data |
BASF Ultramid® 1703-2 BK ND3007 25% Glass Filled PA66 (Conditioned) Ultramid 1703-2 BK ND3007 is a 25% glass reinforced, heat stabilized injection molding nylon 6/6. |
|||
Flexural Modulus | 5.10 GPa | 740 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Valox® K4530 PBT 15% glass reinforced PBT, Hydrolytically stable, High flow, Automotive connectors. |
|||
Flexural Modulus | 5.10 GPa | 740 ksi | ASTM D790 |
Adell RR-18 Copolymer Polypropylene, 40% Glass Reinforced Data provided by Adell Plastics, Inc. |
|||
Flexural Modulus | 5.10 GPa | 740 ksi | ASTM-D790 |
Polyram RamSter PF303G4 PBT, 20% Glass Fiber 20% Glass-fiber reinforced, low viscosity PBT for injection molding applications.Information provided by Polyram Ram On Ind. |