Addcomp ADD-MAX® AS 38 Anti-static masterbatch, LLDPE based

Category Other Engineering Material , Additive/Filler for Polymer
Manufacturer Addcomp
Trade Name ADD-MAX®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Addcomp ADD-MAX® AS 38 Anti-static masterbatch, LLDPE based.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Fields of application: Anti-static masterbatch for olefinicsExamples: Thermoformed and injection molded PP or PE products such as containers and other packaging products. Other applications are films, sheets, tapes, yarns, fibers and household products.Mode of action and advantages: ADD-VANCE AS 38 contains a high concentration of a highly effective synergistic blend of anti-static additives. The combination of internal anti-static agents used in this product reduces the surface resistance of olefinics.Advantages: Immediate anti-static protection after production of the article; The balanced ratio of fast and controlled migrating anti-static additives does not only provide a rapid anti-static effect but also a prolonged protection against dust attraction and other inconveniences caused by electrostatic charging; Surface resistance of less than 1011 Ohm within 24 hours @ 1% dosing rate; Safe to use as a result of the food contact approved anti-static formulation; Excellent de-molding properties for injection molded products; Good cost economy; Non-sticking pellets, dust free dosing; and Safe and easy handling.Regulations: ADD-VANCE AS 38 is very suitable for food packaging products as the active ingredients are in compliance with current food contact regulationsInformation provided by ADDCOMP
Electrical Properties Metric English Comments
Surface Resistance <= 1.00e+11 ohm

@Time 86400 sec
<= 1.00e+11 ohm

@Time 24.0 hour
1% dosing rate
Processing Properties Metric English Comments
Processing Temperature <= 280 °C
<= 536 °F
Descriptive Properties Value Comments
Appearance White/off-white granules
Dosing Level 0.4-1.5%