Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Arkema Group Nakan® RPX 301 L PVC, Rigid Extrusion Grade

Category Polymer , Thermoplastic , Vinyl (PVC) , PVC, Rigid Grade
Manufacturer Arkema
Trade Name Nakan®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Arkema Group Nakan® RPX 301 L PVC, Rigid Extrusion Grade.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
NAKAN RPX 301 L is a rigid polyvinyl chloride compound developed for extrusion of transparent profiles for outdoor applications.ISO data provided by the manufacturer, Arkema.
Physical Properties Metric English Comments
Density 1.36 g/cc
0.0491 lb/in³
Mechanical Properties Metric English Comments
Tensile Strength, Yield 51.0 MPa
7400 psi
50 mm/min
Elongation at Break 45 %
45 %
Nominal Strain; 50 mm/min
Elongation at Yield 5.0 %
5.0 %
50 mm/min
Tensile Modulus 2.53 GPa
367 ksi
1 mm/min
Charpy Impact Unnotched NB
NB
Charpy Impact, Notched 0.580 J/cm²
2.76 ft-lb/in²
Thermal Properties Metric English Comments
Vicat Softening Point 77.0 °C
171 °F
50°C/hr; 50N
Flammability, UL94 V-0

@Thickness 1.60 mm
V-0

@Thickness 0.0630 in
Optical Properties Metric English Comments
Transmission, Visible 90 %
90 %
transparent; thickness not quantified
Copyright © lookpolymers.com All Rights Reserved