Panipol Oy T Inherently Conductive Polymer

Category Other Engineering Material , Additive/Filler for Polymer , Polymer
Manufacturer Panipol
Trade Name Oy
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Panipol Oy T Inherently Conductive Polymer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Doped polyaniline in tolueneSolution Processing, Coating formulations, Ink formulationsInformation provided by Panipol Oy Ltd
Physical Properties Metric English Comments
Solids Content 3.0 - 10 %
3.0 - 10 %
Viscosity 10 - 30 cP
10 - 30 cP
0.5-10.0% solids
Electrical Properties Metric English Comments
Surface Resistivity per Square 1400 - 150000 ohm
1400 - 150000 ohm
Descriptive Properties Value Comments
CAS Number 159996-80-2
Toluene, CAS Number 108-88-3