Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Aclo Accutech Polypropylene Homopolymer HP0334M30CL Mica Reinforced Coupled

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene with 30% Mica Filler
Manufacturer Aclo Compounders
Trade Name Accutech
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Aclo Accutech Polypropylene Homopolymer HP0334M30CL Mica Reinforced Coupled.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Physical Properties Metric English Comments
Density 1.12 g/cc
0.0405 lb/in³
ASTM D792
Linear Mold Shrinkage 0.0070 cm/cm
0.0070 in/in
MD; ASTM D955
Melt Flow 4.0 g/10 min
4.0 g/10 min
ASTM D1238
Ash 30 %
30 %
ASTM D2584
Mechanical Properties Metric English Comments
Hardness, Rockwell R 62
62
ASTM D785
Tensile Strength at Break 27.0 MPa
3920 psi
ASTM D638
Tensile Strength, Yield 35.0 MPa
5080 psi
ASTM D638
Elongation at Break 10 %
10 %
ASTM D638
Elongation at Yield 4.0 %
4.0 %
ASTM D638
Tensile Modulus 3.499 GPa
507.5 ksi
ASTM D638
Flexural Strength 48.0 MPa
6960 psi
ASTM D790
Flexural Modulus 3.499 GPa
507.5 ksi
ASTM D790
Izod Impact, Notched 0.438 J/cm
0.820 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 122 °C
252 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 73.9 °C
165 °F
Users viewing this material also viewed the following: