Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 0.438 J/cm @Temperature 22.8 °C |
0.820 ft-lb/in @Temperature 73.0 °F |
ASTM D256 |
Ensinger Sintimid™ V-HPHT high purity high temp Polyimide (PI)
(discontinued **) SINTIMID™ V polyimide stock shapes provide a superior combination of high temperature and bearing and wear, properties that make it an idea choice for the most demanding applications. SINTIMID™ V.. |
|||
Izod Impact, Notched | 0.438 J/cm | 0.820 ft-lb/in | ASTM D256 |
Aclo Accutech Polypropylene Copolymer HP0334W10L Wollastonite Reinforced |
|||
Izod Impact, Notched | 0.438 J/cm | 0.820 ft-lb/in | ASTM D256 |
Aclo Accutech Polypropylene Homopolymer HP0334G20CL Glass Reinforced Coupled |
|||
Izod Impact, Notched | 0.438 J/cm | 0.820 ft-lb/in | ASTM D256 |
Aclo Accutech Polypropylene Homopolymer HP0334M30CL Mica Reinforced Coupled |
|||
Izod Impact, Notched | 0.438 J/cm | 0.820 ft-lb/in | ASTM D256 |
Aclo Accutech Polypropylene Homopolymer HP0336W10L1 Wollastonite Reinforced |
|||
Izod Impact, Notched | 0.438 J/cm | 0.820 ft-lb/in | ASTM D256 |
Aaron Industries AAROPRENE® CFPP 2030 Calcium Carbonate Filled Polypropylene AAROPRENE® CFPP 2000 Series Reinforced CompoundsMelt flow index may be specified. Color may be specified. |
|||
Izod Impact, Notched | 0.438 J/cm | 0.820 ft-lb/in | ASTM D256 |
Aclo Accutech SAN SAN930G20L Glass Reinforced |