Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Aclo Accucomp Polycarbonate POL052L High Viscosity

Category Polymer , Thermoplastic , Polycarbonate (PC) , Polycarbonate, Molded
Manufacturer Aclo Compounders
Trade Name Accucomp
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Aclo Accucomp Polycarbonate POL052L High Viscosity.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Physical Properties Metric English Comments
Density 1.20 g/cc
0.0434 lb/in³
ASTM D792
Linear Mold Shrinkage 0.0060 cm/cm
0.0060 in/in
MD; ASTM D955
Melt Flow 10 g/10 min
10 g/10 min
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell R 122
122
ASTM D785
Tensile Strength at Break 65.0 MPa
9430 psi
ASTM D638
Tensile Strength, Yield 66.0 MPa
9570 psi
ASTM D638
Elongation at Break 130 %
130 %
ASTM D638
Elongation at Yield 75 %
75 %
ASTM D638
Tensile Modulus 1.80 GPa
261 ksi
ASTM D638
Flexural Strength 97.01 MPa
14070 psi
ASTM D790
Flexural Modulus 2.699 GPa
391.5 ksi
ASTM D790
Izod Impact, Notched 9.50 J/cm
17.8 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 138 °C
280 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 125 °C
257 °F