Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 9.52 J/cm | 17.8 ft-lb/in | ASTM D256 |
Ovation Polymers Opnyl OP66UT119 Nylon 66 Ultra Tough - High Impact, Excellent retention of mechanical properties, High service temperature. *All properties are measured after 48 hours of conditioning at 23°C and 50% relative humidity. All.. |
|||
Izod Impact, Notched | 9.50 J/cm | 17.8 ft-lb/in | ASTM D256 |
Premix Premi-Glas® 1203-30 Fiberglass Reinforced SMC Description: Premi-Glas® 1203-30 is a fiberglass-reinforced, thermoset sheet molding compound designed for structural and semi-structural components where smooth flat surfaces, high strength and st.. |
|||
Izod Impact, Notched | 9.50 J/cm | 17.8 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Lexan® ML6412 PC Copolymer ML6412 is an impact modified PC resin with non-brominated, non-chlorinated flame retardant system. |
|||
Izod Impact, Notched | 9.50 J/cm | 17.8 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Lexan® ML6412 PC Copolymer (Asia Pacific) ML6412 is an impact modified PC resin with non-brominated, non-chlorinated flame retardant system. |
|||
Izod Impact, Notched | 9.50 J/cm | 17.8 ft-lb/in | ASTM D256-70 |
Budd DSM-971 Smooth Surface, Class "A" SMC
(discontinued **) Parts requiring high strength and dimensional stability, excellent surface smoothness without sink marks; parts to be painted requiring an automotive-type finish.Data provided by the manufacturer. |
|||
Izod Impact, Notched | 9.50 J/cm | 17.8 ft-lb/in | ASTM D256 |
IDI Composites A-205 Thermoset Polyester, Sheet AUTOMOTIVE - Versatile family of compounds specifically designed for automotive structural applications. Low shrink characteristics, heat resistance, long-term dimensional stability, and corrosion r.. |
|||
Izod Impact, Notched | 9.50 J/cm @Thickness 3.17 mm |
17.8 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Ineos ABS Triax® 1220 S ABS + Polyamide Blend, Extrusion, Dry as Extruded Properties tested in transverse direction (worst case) on 125-mil (3.2 mm) extruded sheets specimens with |
|||
Izod Impact, Notched | 9.50 J/cm @Thickness 3.20 mm |
17.8 ft-lb/in @Thickness 0.126 in |
ASTM D256 |
Ineos ABS TRIAX® 1220 S ABS/Nylon Blend, Dry as Molded Extrusion and injection molding grade with good stress corrosion cracking resistance, good chemical resistance (fuel, cleaning agents), high impact and notched impact strength, good acoustical dampi.. |
|||
Izod Impact, Notched | 9.50 J/cm @Thickness 3.20 mm |
17.8 ft-lb/in @Thickness 0.126 in |
ASTM D256 |
SABIC Innovative Plastics ULTEM 1285 PEI Transparent Polyetherimide blend. ECO Conforming. US FDA and EU Food Contact Compliant in recognized colors. |
|||
Izod Impact, Notched | 9.50 J/cm @Thickness 3.20 mm |
17.8 ft-lb/in @Thickness 0.126 in |
ASTM D256 |
SABIC Innovative Plastics ULTEM 1285 PEI (Asia Pacific) Transparent Polyetherimide blend. ECO Conforming. US FDA and EU Food Contact compliant in recognized colors. |
|||
Izod Impact, Notched | 9.50 J/cm @Thickness 3.20 mm |
17.8 ft-lb/in @Thickness 0.126 in |
ASTM D256 |
SABIC Innovative Plastics ULTEM DU319 PEI Transparent Polyetherimide blend. ECO Conforming. US FDA and EU Food Contact Compliant in recognized colors. |
|||
Izod Impact, Notched | 9.50 J/cm | 17.8 ft-lb/in | ASTM D265 |
Solvay TECHNYL® 27010ST PA66, DRY Description: Polyamide 66, with very high impact resistance even at low temperature, for injection molding.Available in: Asia PacificProduct Applications: TECHNYL® 2710ST is used in all sector of.. |
|||
Izod Impact, Notched | 9.50 J/cm | 17.8 ft-lb/in | ASTM D256 |
Aclo Accucomp Polycarbonate POL052L High Viscosity |