2-part solvent-free dielectric epoxy casting compound.Processing: 100/50 ratio (pbw); Gel time, 100 g (3.5 oz.): 480 minutes; cures in 3 weeks at 25°C (77°F).Applications: solventless casting, adhesive, and coating.
Physical Properties Metric English Comments
Water Absorption 0.31 %
0.31 %
in 24 hours.
Viscosity Measurement 445
445
Mechanical Properties Metric English Comments
Hardness, Shore D 80
80
Tensile Strength, Ultimate 45.51 MPa
6601 psi
Elongation at Break 18 %
18 %
Flexural Strength 76.88 MPa
11150 psi
Electrical Properties Metric English Comments
Electrical Resistivity 2.90e+9 ohm-cm

@Temperature 93.3 °C
2.90e+9 ohm-cm

@Temperature 200 °F
2.40e+11 ohm-cm

@Temperature 65.6 °C
2.40e+11 ohm-cm

@Temperature 150 °F
3.60e+15 ohm-cm

@Temperature 25.0 °C
3.60e+15 ohm-cm

@Temperature 77.0 °F
Dielectric Constant 3.26

@Frequency 1e+6 Hz
3.26

@Frequency 1e+6 Hz
Dissipation Factor 0.011

@Frequency 1e+6 Hz
0.011

@Frequency 1e+6 Hz
Processing Properties Metric English Comments
Processing Temperature 25.0 °C
77.0 °F
Curing time: 3 weeks