Polymer Property : Electrical Resistivity = 2.40e+11 ohm-cm Product List

Electrical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Electrical Properties Metric English Comments
Electrical Resistivity 2.40e+11 ohm-cm

@Temperature 65.6 °C
2.40e+11 ohm-cm

@Temperature 150 °F
Abatron AboCast 8-9/Abocure 8-9 Epoxy  (discontinued **)
2-part solvent-free dielectric epoxy casting compound.Processing: 100/50 ratio (pbw); Gel time, 100 g (3.5 oz.): 480 minutes; cures in 3 weeks at 25°C (77°F).Applications: solventless casting, adh..
Electrical Resistivity 2.40e+11 ohm-cm

@Temperature 93.3 °C
2.40e+11 ohm-cm

@Temperature 200 °F
Abatron AboCast 8-15/Abocure 8-15 Epoxy  (discontinued **)
2-part, clear, solvent-free dielectric epoxy casting compound.Processing: 100/11.80 ratio (pbw); Gel time, 100 g (3.5 oz.): 70 minutes; cures in 16 hours at 25°C (77°F); postcure: 2 hours at 100°..